| DISTRIBUTION OF NON-METALLIC INCLUSIONS IN RIMMING STEEL INGOTS |
| SHIH CHANG-HSU;LEE CHIN-YUAN Institute of Metal Research; Academia Sinica |
|
Cite this article:
SHIH CHANG-HSU;LEE CHIN-YUAN Institute of Metal Research; Academia Sinica. DISTRIBUTION OF NON-METALLIC INCLUSIONS IN RIMMING STEEL INGOTS. Acta Metall Sin, 1957, 2(2): 153-168.
|
|
|
Abstract The distribution and types of non-metallic inclusions in rimming steel ingotsobtained by four different teeming practices have been investigated microscopically.The different teeming practices were: (1) ordinary, (2) slag covering, (3) coveredtop of ingot mould during teeming, and (4) same as in (3), but immediately afterthe completion of teeming, a heavy steel plate was placed on top of the moltenmetal. Quantitative results indicate that the types and distribution of non-metallicinclusions in these ingots are basically similar, except that oxide networks alonggrain boundaries were observed in ingots obtained by using the last three teemingpractices. Several interesting phenomena are revealed and discussed. Suggestionsto improve the teeming practice are given.
|
|
Received: 18 February 1957
|
[1] 吕湘提,胡文淦,甘克先,改善沸腾钢钢锭质量的研究,本期金属学报. [2] Hultgren, A. and Phragmen G., Trans. AIME, 133 (1939) , 133. [3] Swinden, T., Jour. Iron and steel Inst., Spec. Rop., No. 27, 17. [4] (1955) , 382--413. [5] Washburn, T. S. and Nead, J. H., Trans. AIME. 125 (1937) , 378. [6] (1953) ,吴昌衡,李静媛,李代钟,徐思盛译,钢中夹杂物的金相鉴定,(1956) ,科学出版社. [7] ASM Metals Handbook(1948) , 445--452. [8] 庄育智,吴昌衡,金属学报,第一卷第二期,1956年6月,155. [9] 李董,陈继志等,金属学报,第一卷第四期,1956年12月. [10] Whiteley, J. H., 7th Rop. on Steel Ingots, Inst. of Iron and Steel Spec. Rep., No. 16(1937) , 23. [11] Sims, C. H., Proc. Electric Furn. Steel, 10 (1952) , 152. [12] Dickson, J. H. S. Jour. Iron and Steel Inst., 113 (1926) , 177. [13] Herty, C. H. and Fitterer, G. R., Trans. Am. Soc. Steel Treat., 15 (1929) , 569. [14] 赵淑熙,李静媛 未发表的报告,1956年12月. [15] Rait, J. R. and Pinder, H. W, Jour. of Iron and Steel Inst., 154 (1946) , 371. [16] Morton, A. L. and Carter, P. T., Jour. of Scot. Iron and Steel Inst., 59 (1951-52) , 96. [17] Hayes, A. and Chipman, J., Trans. AIME, 135 (1939) , 85. [18] (1950) , [19] (1950) , № 4, 311. [20] A training course from United States Steel Corporation. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|