THE RECRYSTALLIZATION AND MAGNETIC PROPERTIES OF ARMCO IRON
TAI LI CHI(L.C.TAI)Research Institute of Iron and Steel
Cite this article:
TAI LI CHI(L.C.TAI)Research Institute of Iron and Steel. THE RECRYSTALLIZATION AND MAGNETIC PROPERTIES OF ARMCO IRON. Acta Metall Sin, 1958, 3(3): 227-230.
Abstract The microstructure and the magnetic properties of cold reduced and annealed armco iron arestudied.The textures of the samples used in the experiments have been determined by the X-raypole figure and the magnetic torque methods as reported in the two earlier papers.The samples having higher magnetic permeabilities show a secondary recrystallization.Therelations between recrystallization and magnetic properties are briefly discussed.