Please wait a minute...
Acta Metall Sin  1959, Vol. 4 Issue (1): 60-68    DOI:
Current Issue | Archive | Adv Search |
THE RECTANGULAR HYSTERESIS LOOP OF GRAIN ORIENTED NICKEL-IRON ALLOY
TAI LI-CHI (L. C. TAI);LIU REN-PAO;WANG LI-KO Iron and Steel Research Institute; Peking North-East Peoples University; Changchun
Cite this article: 

TAI LI-CHI (L. C. TAI);LIU REN-PAO;WANG LI-KO Iron and Steel Research Institute; Peking North-East Peoples University; Changchun. THE RECTANGULAR HYSTERESIS LOOP OF GRAIN ORIENTED NICKEL-IRON ALLOY. Acta Metall Sin, 1959, 4(1): 60-68.

Download:  PDF(872KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The D. C. and A. C. methods are used for the measurement of the magnetic properties of 50pct. nickel and 50 pct. iron Ni-Fe alloy. The ratio between the remanence and the magneticsaturation induction, B_r/B_s, and the coercive force, H_c, are taken as a criterion for assessing themagnetic characteristics of the alloy. The samples used in the experiments are cold-rolled with (Ⅰ) 94 per cent, (Ⅱ) 98 per cent and(Ⅲ) 99 per cent reductions. The class Ⅰ and class Ⅱ samples are annealed at (1) 900°, (2) 1000°, (3)1100°, (4) 1200° and (5) 1300℃ for one hour. The class Ⅲ samples are annealed at 1100℃ for(1) 30 minutes, (2) one hour, and (3) one and half an hour respectively. The formation of the cubic texture of the alloy has been studied by the X-ray pole figuremethod and the results Will be presented in another paper. The development of the material used for the magnetic amplifiers is finally discussed.
Received:  18 January 1959     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1959/V4/I1/60

[1] Six. W., Snoek, J. L., Burgers, W. G., Der Ingenieur, 49 (1934) , E195.
[2] Becker, R., Doring, W., Ferromagnetismus. (1939) , S. 431.
[3] Pawlek, F., Z. Metallkunde, 27 (1935) , 160.
[4] Crede, J. H., Martin, J. P., Journ. app. Phys., 20 (1944) , 966.
[5] Seymour, W. E., Harker, D., Trans. AIME, 188 (1950) , 1001.
[7] Розенблат,М.А,Магнитние Усилители,(1955) ,译本“磁放大器”,人民邮电出版社(1958) .
[8] 地内骏,田中满,日本材料试验,由气材料特集号,41(1957) ,78.
[9] Ward, C. E., Littmann, M. F., Trans. AIEE, 74 (1955) , 422.
[10] Кифер, И. И., Пантюшин, В. С., (1955) , 179.
[11] Pawlek, F., Magnetische Werkstoff, (1953) , S. 196.
[12] Dahl, O., Pawlek, F., Z. Metallkunde, 28 (1936) , 266.
[13] Dahl, O., Pawlek, F., Z. fur Physik, 94 (1935) , 504.
[14] Rathenau, G. W., Custers. J. F. H., Philipps Res. Rep., 4 (1949) , 241.
[15] Wassermann, G., Z. Metallkde., 28 (1936) , 262.
[16] Kronberg, W. L., Wilson, F. H., Journ. of Metals, 185 (1949) , 501.
[17] 戴礼智、张信钰,刘壬宝,金属学报,4(1959) ,52.
No related articles found!
No Suggested Reading articles found!