Acta Metall Sin  1959, Vol. 4 Issue (3): 262-269    DOI:
Current Issue | Archive | Adv Search |
THE TEMPER-BRITTLENESS OF BAINITIC STEELS
TAN YU-HUA Anshan Institute of Iron and Steel Technology
Cite this article: 

TAN YU-HUA Anshan Institute of Iron and Steel Technology. THE TEMPER-BRITTLENESS OF BAINITIC STEELS. Acta Metall Sin, 1959, 4(3): 262-269.

Download:  PDF(715KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A study of the occurrence of temper-brittleness in bainitic structure has been made. It wasfound that the tendency of temper-embrittlement in the lower bainite was slightly less than thatin the tempered martensite whik the temper-embrittlement in the upper bainite was slightly greaterthan that in pearlitic structure, and the tendency of temper embrittlement of the temperedmartensite was much greater than that of the pearlite. The temperature range of temper-brittleness was 460—580℃ for upper bainite, 430—620℃ for tempered martensite, and the tem-perature of maximum temper-embrittlement appeared to be about 530℃ for both. It was sug-gested that the mechanism of temper-brittleness is the same for both structures.
Received:  18 March 1959     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1959/V4/I3/262

[1] R. H. Grenves and J. A. Jones: J. Iron Steol Inst., 1920, 102, 171.
[2] Н. Н. Минкевич: ЖРМО, 1927, № 1, 52.
[3] E. Mnurer, O. H. Wilms und H. Kiassler: Stahl und Eisen, 1942, 62, 81.
[4] W. S. Pellini and B. R. Queneau: Trans. A. S. M., 1947, 39, 139.
[5] B. C. Woodfine: J. Iron Steel Inst., 1953, 173, 229.
[6] N. P. Allen and C. C. Eanley: ibid., 1956, 182, 375.
[7] Т. В. Сергиевская: Сталь, 1955, № 1, 63.
[8] D. C. Buffum and L. D. Jaffe: Trans. A. I. M. E., 1953, 197, 1373.
[9] Atlas of Isothermal Transformation Diagrams, 19.
[10] Н. Т. Гулцова, М. Л. Бернщтейна, А. Г. Ражштадта: 1956, 436.
[11] Л. В. Смирнов, Д. Д. Садовский: 1956.
[12] В. А. 捷列:合金构钢,重工业出版社,1956.
[13] С. Т. Кишкин: 1941, № 4, 91.
[14] Л. С. Ольховой и Д. Я. Вишняко: 1956, 36.
[15] D. McLean and L. Northcott. J. Iron Steel Inst., 1948, 158, 169.
[16] В. И. Архаров: 1946, 8; 1955, 16.
[17] R. Maloof: Trans. A. S. M., 1952, 44, 264; 或 1953, № 3, 121.
[18] Н. В. Казакова, Н. В. Королева: 1955, 105, № 6, 1233.
[19] С. Ф. Юрьев: 1956, № 10, 37.
[20] H. A. Dichie: Stahl und Eisen, 1928, 48, 50.
[21] Honda Katar: Metal Ptogress, 1933, (6) , 43.
[22] А. Н. Ризоль, Л. Г. Сакварелдзе и Л. М. Утевский: 1955, 105, 268.
[23] 雄井英雄:日本金属学会会志,1956(10) ,20,550.
[24] А. С. Завьяков, Л. Я. Гольдштейн и М. И. Сенченко: 1957.
[25] J. H. S. Dickensan: J. West. Scotland, Iron Stoel Inst., 1919, 110.b
No related articles found!
No Suggested Reading articles found!