Please wait a minute...
Acta Metall Sin  1963, Vol. 6 Issue (2): 131-145    DOI:
Current Issue | Archive | Adv Search |
AN INVESTIGATION ON THE RESISTANCE TO PLASTIC DEFORMATION OF MILD STEEL,13% CHROMIUM STEEL,ALUMINIUM AND LEAD AT DIFFERENT TEMPERATURES AND AT VARIOUS RATES OF STRAIN
CHANG TSO-MEI;CHAO SHIH-TA Institute of Optics & Fine Mechanics;Academia Sinica
Cite this article: 

CHANG TSO-MEI;CHAO SHIH-TA Institute of Optics & Fine Mechanics;Academia Sinica. AN INVESTIGATION ON THE RESISTANCE TO PLASTIC DEFORMATION OF MILD STEEL,13% CHROMIUM STEEL,ALUMINIUM AND LEAD AT DIFFERENT TEMPERATURES AND AT VARIOUS RATES OF STRAIN. Acta Metall Sin, 1963, 6(2): 131-145.

Download:  PDF(3374KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Homogeneous compression tests were carried out in a cam plastometer on mild steel,13% chromium steel,aluminium and lead.Aluminium and lead were tested at roomtemperatures;while mild steel and 13% chromium steel were tested at 1000,1100 and1200℃.Altogether five different rates of strain were used,ranging from 12.2 sec.~(-1)to 183 sec.~(-1),the rate of strain being kept constant during the test.With the exceptionof lead,which reached a reduction of 76%,the maximum reduction in height was 56%.During the tests,the testing temperatures were controlled accurately.The friction be-tween the specimen and the compression platens was successfully eliminated,so that testswere carried out under homogeneous compression conditions,and the true stress-straincurves corresponding to the above testing conditions were thus obtained.The experimental results show that under the above testing conditions the relation-ship between the rate of strain and the resistance to deformation for mild steel,13%chromium steel and lead obeys the following law(?)while the stress-strain curves for aluminium is practically unaffected by the change in theabove rates of strain.These experimental results have been discussed and compared withprevious work found in literature.
Received:  18 February 1963     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1963/V6/I2/131

[1] Manjoine,M.J.,Nadai,A.:Proc.Am.Soc.Testing Mater.,1940,40,822.
[2] Nadai,A.,Manjoine,M.J.:J.Appl.Mech.,1941,6,A77.
[3] 丰岛清三:铁と钢,1955,41,344.
[4] #12
[5] 井上胜郎:铁と钢,1955,41,506;41,593.
[6] Chang Tso-mei(张作梅),Shü,U-yung(徐有容):Sci.Sinica,1961,10,377.
[7] Alder,J.F.,Phillips,V.A.:J.Inst.Metals,1954-1955,83,80.
[8] Cook,P.M.:Proccedings of the Conference on the Properties of Materials at High Rates of Strain,(IME,1957) ,p.86-97.
[9] Loizou,N.,Sims,R.B.:J.Mech.Phys.Solids,1952-1953,1-2,237.
[10] 松浦佑次:日本机械学会志,1959,62,1387.
[11] Hockett,J.E.:Proc.Am.Soc.Testing Mater.,1959,59,1309.
[12] #12
[13] #12
[14] #12
[15] Fink,K.,Lueg,W.,Bürger,G.:Arch.Eisenhüttenw.,1955,655.
[16] 桥爪伸:日本机械学会志,1959,62,1392。
[17] 朱云青、丁安华:全国实验应力分析第一次报告会文献汇编,(科学出版社,1959年),95-106页.
[18] 井上胜郎:机械研究,1958,10,25。
[19] 张作梅、孙麟治:机械工程学报,1957,5,329。z
No related articles found!
No Suggested Reading articles found!