Please wait a minute...
Acta Metall Sin  1965, Vol. 8 Issue (3): 319-325    DOI:
Current Issue | Archive | Adv Search |
DIFFUSION OF COBALT IN COPPER SINGLE CRYSTALS
TSIEN CHIH-CHIANG;KAO SHU-CHUN;CHANG PEI-LIN Institute of Metal Research; Academia Sinica
Cite this article: 

TSIEN CHIH-CHIANG;KAO SHU-CHUN;CHANG PEI-LIN Institute of Metal Research; Academia Sinica. DIFFUSION OF COBALT IN COPPER SINGLE CRYSTALS. Acta Metall Sin, 1965, 8(3): 319-325.

Download:  PDF(611KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The experimental details of the determination of diffusion coefficients by the"residual activity" method are described. The possible sources of errors are discussed.The diffusion coefficient of Co~(60) in copper single crystals determined by this method isgiven as D=0.84 exp (-52,100/RT) cm~2/sec which is in good agreement with the resultsof Macklietl and Sakamoto obtained by "sectioning method".
Received:  18 March 1965     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1965/V8/I3/319

[1] Tomizuka, C. T.: Methods of Bxperimental Physics, ed. K. Lark-Horovitz, (Academic, 1959) , vol. 6, pt. A, p. 364.
[2] #12.
[3] Mortlock, A. J., Tomlin, D. H.: Proc. Phys. Soc., 1956, B69, 250.
[4] Smith, R. L., Jaumot, F. E., Arne, L. A.: Phys. Rev., 1954, 94, 1407.
[5] #12.
[6] Letaw, H., Slifkin, L. M., Portnoy, W. M.: Rev. Sci. Instr., 1954, 25, 865.
[7] Messner, A., Benson, R., Dorn, J. E.: Trans. Am. Soc., Metals, 1961, 53, 227.
[8] Peart, R. F., Tomlin, D. H.: Acta Met., 1962, 10, 123.
[9] Peart, R. F., Graham, D., Tomlin, D. H.: Acta Met., 1962, 10, 519.
[10] Mackliet, C. A.: Phys. Rev., 1958, 109, 1964.
[11] Sakamoto, M.: J. Phys. Soc. Japan, 1958, 13, 845.
[12] Styris, D. L., Tomizuka, C. T.: J. Appl. Phys., 1963, 34, 1001.
[13] Schamp, H. W., Oakes, D. A., Reed, N. M.: Rev. Sci. Instr., 1959, 30, 1028.