| AN INVESTIGATION ON AN AUSTENITIC Fe-Mn-Al HEAT-RESISTING STEEL |
| CHANG YEN-SHEN;SHIH CHANG-HSU;LI YOU-K'E |
|
Cite this article:
CHANG YEN-SHEN;SHIH CHANG-HSU;LI YOU-K'E. AN INVESTIGATION ON AN AUSTENITIC Fe-Mn-Al HEAT-RESISTING STEEL. Acta Metall Sin, 1965, 8(3): 346-430.
|
|
|
Abstract On the basis of our previous investigation, an Fe-Mn-Al steel containing 29.4%Mn, 3.8% Al, 1.9% Mo, 0.5% V, 0.4% W, 0.015% B, 0.03% N and 0.1% C hasbeen studied systematically. Its workability is similar to that of 1Cr_(18)Ni_9Ti. The stress-rupture properties arecomparable to those of high Cr-Ni austenitic steels, such as ЭИ257Т (14% Cr, 14% Ni,2.15% W, 0.5% Mo, 0.5% Ti, 0.1% C) at 600°and 650℃ for several thousandhours. On ageing at temperatures from 600°to 750℃ for periods up to 9500 hours, ac-companied by changes in hardness, the following phases appeared with increasing ageingtime and temperature: γ V_4C_3, M_6C and AB_2 (Laves phase). The impact value de-creased from about 37 to 10 kg·m/cm~2 after 9500 hours at 650°and 700℃.
|
|
Received: 18 March 1965
|
[1] 张彦生、师昌绪:金属学报,1964,7,285. [2] #12. [3] #12. [4] #12. [5] Beattie, H. J., VerSnyder, F. L.: Trans. Am. Soc. Metals, 1953, 45, 397. [6] 拉施柯,H.Ф.著,钢铁研究院译:奥氏体钢的相分析及其组织,(冶金工业出版社,1959年),198页. [7] 李有柯、谢仰华、郭蕴宜等:铬锰氮奥氏体耐热钢的研究,待发表. [8] 郭蕴宜:铬锰氮奥氏体耐热钢的时效脆性,待发表. [9] Gemmill, M. G., Hughes, H., Murray, J. D. et al.: J. Iron Steel Inst. (London), 1956, 84, 122. [10] #12. [11] #12. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|