Export:  BibTeX | EndNote (RIS)      
Abstract  The nucleation process in the pearlite range is additive, except that holding in thelower pearlite range it tends to accelerate subsequent reaction at high temperature. Inthe bainite range, holding at a high temperature retards subsequent nucleation at a lowtemperature, while holding at a low temperature appears to accelerate subsequent nuclea-tion at a high temperature. The deviation from additivity depends upon difference be-tween the temperatures involved and the holding duration. It is suggested that the embryo of bainite is the same as that of martensite, i. e., ab. c. c. region surrounded by a dislocation loop. Holding in the lower pearlite range accelerates subsequent transformation to bainite.
Received:  18 March 1965     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1965/V8/I3/360

[1] Hollomon, J. H., Jaffe, L. D., Norton, M. R.: Trans. AIME, 1946, 167, 419.
[2] Jaffe, L. D.: Trans. AIME, 1948, 176, 363.
[3] Moore, P. T.: J. Iron Steel Inst. (London), 1954, 177, 305.
[4] Hehemann, R. F., Troiano, A. R.: Trans. AIME, 1954, 20O, 1272.
[5] #12.
[6] #12.
[7] #12.
[8] White, J. S., Owen, W. S.: J. Iron Steel Inst. (London), 1961, 197, 241.
[9] Jolivet, H., Portevin, A.: Compt. Rend., 1939, 209, 379, 556.
Jo1ivet, H., Portevin, A.: Genie Civil, l939, 115, 464, $N [1] .
[10] Gordon, P., Cohen, M., Rose, R. S.: Trans. Am. Soc. Metals, 1943, 31, 161.
[11] Lyman, T., Troiano, A. R.: Trans. AIME, 1945, 162, 196.
[12] 何俊:金属和合金的马氏体型相变,1961年,全国第一次金属物理学术会议.
[13] Kaufman, L., Cohen, M.: Progress in Metal Physics, (Pergamon, 1958) , vol. 7, p. 165--246.
[14] Goodenow, R. H., Matas, S. J., Hehemann, R. F.: Trans. AIME, 1963, 227, 651.
No related articles found!
No Suggested Reading articles found!