Abstract The results of tension, compression and plastic bending tests made on a Hadfield steel have been compared, from which a quantitative relationship between them has been found. It is suggested that plastic bending test may either be used as an independent test or as an estimation for the direct tension and compression tests. The correlation between them may be used to explain the technical specifications for cast products of Hadfield steel.
|