Please wait a minute...
Acta Metall Sin  1965, Vol. 8 Issue (4): 545-548    DOI:
Current Issue | Archive | Adv Search |
APPLICATION OF THE θ FUNCTION TO THE MODIFIED GIBBS-DUHEM EQUATION
CHOU KUO-CHIH (Peking Institute of Ferrous Metallurgy)
Cite this article: 

CHOU KUO-CHIH (Peking Institute of Ferrous Metallurgy). APPLICATION OF THE θ FUNCTION TO THE MODIFIED GIBBS-DUHEM EQUATION. Acta Metall Sin, 1965, 8(4): 545-548.

Download:  PDF(217KB) 
Export:  BibTeX | EndNote (RIS)      