EVALUATION OF BRITTLENESS OF THE NITRIDING COATING IN SOME STEEL BY ACOUSTIC EMISSION TECHNIQUE
"Three-in-One" Res. Gp. of Peking Institute of Iron and Steel Technology; Research Institute of Peking Machine Tools Works and Institute of Metal Research
Cite this article: 

"Three-in-One" Res. Gp. of Peking Institute of Iron and Steel Technology; Research Institute of Peking Machine Tools Works and Institute of Metal Research. EVALUATION OF BRITTLENESS OF THE NITRIDING COATING IN SOME STEEL BY ACOUSTIC EMISSION TECHNIQUE. Acta Metall Sin, 1977, 13(z1): 139-144.