| AN INVESTIGATION OF CASSITERITE FLOTATION USING MIXED TOLYL ARSONIC ACID |
| Res. Gp. of Cassiterite Flotation; Changsha Institute of Mining and Metallurgy Research |
|
Cite this article:
Res. Gp. of Cassiterite Flotation; Changsha Institute of Mining and Metallurgy Research. AN INVESTIGATION OF CASSITERITE FLOTATION USING MIXED TOLYL ARSONIC ACID. Acta Metall Sin, 1978, 14(1): 17-26.
|
|
|
Abstract The capacity of tolyl arsonic acids for collecting cassiterite has been investigated. It is shown that mixed tolyl arsonic acid was much superior to either para- or ortho-isomer alone for cassiterite flotation. Mixing ratios between paraand ortho-tolyl arsonic acids ranging from 50:50 to 30:70 were effective with a peak value at 45:55 in which a maximum collecting capacity was obtained. The preparation of mixed tolyl arsonic acid was more convenient than that of paraisomer, a conventional collecting agent for cassiterite flotation. In the plantscale flotation of cassiterite slimes assaying from 0.6 to 0.7 percent Sn, tin concentrates with the grade of about 25.65% were obtained, the total recovery being about 58.64%. Cassiterite flotation using mixed tolyl arsonic acid as collectors and sodium carbonyl methyl cellulose as despressing agents for calcite have already been put into industrial practice.
|
|
Received: 18 January 1978
|
[1] Topfer, E., Freiber. Forschungsh., [Reihe] A163 (1960) , 63. [2] Anon, World Mining, 26 (1973) , No. 5, 43. [3] Wottgen, E., Freiber. Forschungsh., [Reihe] A551 (1975) , 1. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|