					Cite this article:
						|  |  
    					|  |  
    					| A CRYSTALLOGRAPHIC INVESTIGATION OF A Mg-Ga ALLOY DURING AGING |  
						| Xu Jing-yang and Xu Shun-sheng (Hsu Shun-sheng) (Shanghai Institute of Metallurgy; Academia Sinica) |  
						|  |  
					
			      Xu Jing-yang and Xu Shun-sheng (Hsu Shun-sheng) (Shanghai Institute of Metallurgy; Academia Sinica). A CRYSTALLOGRAPHIC INVESTIGATION OF A Mg-Ga ALLOY DURING AGING. Acta Metall Sin, 1978, 14(2): 139-229.	
				 
					
						| 
								
									|  
          
          
            
              
				
												  
													
													    |  |  
														| Abstract  A crystallographic investigation of a Mg 6%Ga alloy during aging was performed by X-ray diffraction methods, together with hardness measurements and metallographic observations, The aging process of this alloy at 190℃ may be devided into three staps:1. Precipitation of β′. An orthorhombic transition phase β′ is precipitated at the initial stage of aging. Its lattice constants are: aβ′=9.1(?), bβ′=6.2(?), cβ′=24.6(?), and the orientation relationships with the matrix (M) are aβ′∥[0001]M, bβ′∥[2(?)0]M, cβ′∥[01(?)0]M.A preliminary determination showst hat the thin plates of the transition phase are parallel with {10(?)0} and {11(?)0} planes of the matrix.2. Precipitation of β. The equilibrium phase β precipitated out in a Widmanstatten form in the matrix has a composition of Mg_5Ga_2, with lattice constants aβ=13.72(?), bβ=7.02(?), cβ= 6.02(?). The orientation relationships between β and the matrix are: aβ/[0001]M, bβ∥[2110]M, cβ∥[0110]M. Dispersion hardening always accompanies this precipitation, and the habit plane in the matrix was found to be (0001)M.3. Overaging. The Widmanstatten structure of the equilibrium phase in the matrix disappears, and there is no definit orientation relationship between β and the matrix. |  
															| Received:  18 February 1978 |  
            
									            
									               
																												  
															| [1] Pusin, N. A. and Micic, O. D., Z. Anorg. Allg. Chem., 234 (1937) , 229. [2] Roberts, C. S., Magnesium and Its Alloys, Wiley, New York, 1960.
 [3] Pearson, W. B., A Handbook of Lattice Spacings and Structures of Metals and Alloys, Pergamon, London, 1958.
 [4] 长岛晋一,日本金属学会誌,22(1958) ,613;23(1959) ,381,460,465.
 [5] Barrett, C. S., Geisler, A. H. and Mehl, R. F., Trans. AIME, 152 (1943) , 201.
 [6] Henes, S. and Gerold, V., Z. Metall., 53 (1962) , 703.
 [7] Sturkey, L. and Clark, J. B., J. Inst. Metals, 88 (1959-60) , 177.
 [8] Murakam, Y., Kawano, O. and Tamura, H., Mere. Fac. Eng., Kyoto Univ., 24 (1962) , 93. Met. Abstr., 30 (1962) , 192.
 [9] Geisler, A. H. and Hill, J. A., Acta Crystallogr., 1 (1948) , 238.
 [10] #12
 [11] 许顺生,金属X射线学,上海科学技术出版社,1962,p.379.
 [12] Geisler, A. H., Phase Transformations in Solids, Wiley, New York, 1951, p. 387.
 [13] 许顺生等,私人通讯.
 [14] Silcock, J. M., Heal, T. J. and Hardy, H. K., J. Inst. Metals, 82 (1953-54) , 239.
 [15] Hardy, H. K. and Heal, T. J., Progress in Metal Physics, Vol. 5, Butterworths, London, 1954, p. 143.
 [16] 胡素辉,苏千武,许顺生,金属学报,8(1965) ,475.
 [17] Tsuneo Takahashi, Yo Kojima and Kiyoshi Takanishi, J. Japan Inst. Light Metals, 23 (1973) , 376.
 |  
             
								                
															
																| 
																																																																									