Acta Metall Sin  1978, Vol. 14 Issue (4): 420-429    DOI:
Current Issue | Archive | Adv Search |
AN EXPERIMENTAL STUDY ON THE CORRELATION BETWEEN J-INTEGRAL AND STRAIN ENERGY
Wu Xi-jun Jiang Jian Yin Hua-zi (Institute of Metal Research; Academia Sinica)
Cite this article: 

Wu Xi-jun Jiang Jian Yin Hua-zi (Institute of Metal Research; Academia Sinica). AN EXPERIMENTAL STUDY ON THE CORRELATION BETWEEN J-INTEGRAL AND STRAIN ENERGY. Acta Metall Sin, 1978, 14(4): 420-429.

Download:  PDF(743KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  In order to verify the correlation between J-integral and strain energy previously put forward (Acta Metallurgica Sinica, 12, 1976, 162), J_(Ic) values have been determined experimentally by means of TPB type specimens with two different ratios of S/W(4 and 8). The J_(Ic) values obtained by formulaJ=2/B(W-a)(U-U_0+M~2φ/BE'W~2) are: 124-0.5 or 11.7±0.8kg/mm for S/W=4 or 8 and a/W=0.22 to 0.71 or 0.28 to 0.53 respectively. This mesns that similar J_(Ic) values are obtained from TPB specimens of different ratios S/W and a/W. It is further shown that the formula aforementioned contributes a general correlation between J-integral and strain energy.
Received:  18 April 1978     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1978/V14/I4/420

[1] Rice, J. R., J. Appl. Mech., 35 (1968) , 379.
[2] Landes, J. D. and Begley, J. A., Amer. Soc. Test. Mater., Spec. Tech. Publ., № 560, (1974) , p. 170.
[3] 陈篪等,科学通报,20(1975) ,329.
[4] 金属研究所断裂研究组,金属学报,12(1976) ,162.
[5] 金属研究所断裂研究组,金属学报,13(1977) ,122.
[6] Brown, W, F, and Srawley, J. E., Amer. Soc. Test. Mater., Spec. Tech. Publ., № 410, (1967) , p. 13.
[7] Srawley, J. E., Int. J. Fract., 12 (1976) , 475.
[8] 中国科学院北京力学研究所断裂力学研究组,力学,3(1975) ,132
No related articles found!
No Suggested Reading articles found!