ON THE FORMATION OF AMORPHOUS SOLIDS
Zheng Zhaobo Dept;of Physics; University of Science and Technology of China
Cite this article: 

Zheng Zhaobo Dept;of Physics; University of Science and Technology of China. ON THE FORMATION OF AMORPHOUS SOLIDS. Acta Metall Sin, 1979, 15(1): 155-166.

Download:  PDF(1009KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A general survey on theories of glass or amorphous solid formation, includingthe nature of glass transformation, the theory of free volume and that of entropy,the capability on the retention of the amorphous state as well as methods for de-termining the necessary critical cooling rates etc., has been carried out. The re-sults of kinetic treatment of amorphous solid formation shown by D. Turnbulland D. R. Uhlman and their co-workers have received particular attention.
Received:  18 January 1979     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1979/V15/I1/155

[1] Vogel, W., J. Non-Cryst. Solids, 25 (1977) , 179.
[2] Cohen, M. H. and Turnbull, D., J. Chem. Phys., 31 (1959) , 1164.
[3] Turnbull, D. and Cohen, M. H., J. Chem. Phys., 34 (1961) , 120.
[4] Turnbull, D. and Cohen, M. H., J. Chem. Phys., 52 (1970) , 3038.
[5] Gibbs, J. H. and DiMarzio, E. A., J. Chem. Phys., 28 (1958) , 373.
[6] Adam, G. and Gibbs, J. H., J. Chem Phys., 43 (1965) , 139.
[7] Gutzow, I., in "Amorphous Materials", Proc. Ⅲ Int. Conf. Non-Crystalline Solids, 1972, Wiley, London, p. 159.
[8] Uhlmann, D. R., J. Non-Cryst. Solids. 25 (1977) , 42.
[9] Turnbull, D., Contemp. Phys., 10 (1969) , 473.
[10] Hruby, A., Czech. J. Phys., B22 (1972) , 1187.
[11] Vreeswijk. J. C. A. et al., J. Non-Cryst. Solids, 16 (1974) , 15.
[12] Gutzow. I. and Iavvamov, J. Non-Cryst. Solids. 16 (1974) , 128.
[13] Turnbull, D. and Cohen, M. H, J. Chem. Phys., 29 (1958) , 1049.
[14] Duwez, P., Willens, R. H. and Klement, W., J. Appl. Phys.. 31 (1960) , 1136.
[15] Sarjeant. P. T. and Roy. R.. Mater. Res. Bull., 3 (1968) . 265.
[16] Uhlmann. D. R., J. Non-Cryst. Solids, 17 (1975) . 266.
[17] Onorato. P. I. K. and Uhlmann, D. R., J. Non-Cryst. Solids, 7 (1972) , 337.
[18] Davies, H. A., J. Non-Cryst. Solids, 17 (1975) , 266.
[19] Clsvaguera, N., J. Non-Cryst. Solids, 22 (1976) , 23.
[20] Tauc, J., Amorphous and Liquid Semiconductors, Plenum, New York. 1974, pp. 1-39.
No related articles found!
No Suggested Reading articles found!