Joint Res. Gp. of Corrosion; Shanghai Institute of Iron and Steel Research & Changchun Institute of Applied Chemistry; Academia Sinica. THE BEHAVIOUR OF ALLOYING ELEMENTS IN MARINE LOW-ALLOY STEELS Ⅱ. THE INFLUENCE OF ALLOYING ELEMENTS ON THE LOCALISED CORROSION PROPERTY OF LOW-ALLOY STEELS IN ARTIFICIAL SEAWATER. Acta Metall Sin, 1979, 15(2): 227-234.
|
|
|
Abstract The effect of the alloying elements on localised corrosion properties of low-alloy steels has been studied by simulation of an occluded anode cell. Si or Alshowed very strong beneficial main-effect, and at the same time often exerted im-portant influence on the behaviour of other elements. In the latter respect, Si wasthe stronger of the two. The beneficial effect of Cr was marked when the Si con-tent was low (0.1-0.2%), and completely disappeared when Si was increased to0.8-1.0%. Cu behaved somewhat opposite to that of Cr. Mo promoted the benefi-cial effect of Si or Cr, although the main effect of itself alone was unbeneficial.The main effect of Ni is weak, however, it could match with Cu, Mo and Cr-Alto yield beneficial results. With regard to the two elements which were present insteel only in small amount, V was preferable to Nb.
|
|
Received: 18 February 1979
|
[1] Wranglen, G., Corros. Sci., 14 (1974) , 331. [2] Hidega Okada and Heruo Shimada, Corrosion, 30 (1974) , 97. [3] Janik-Czachor, M., Szummer, A. and Szklarska-Sialowska, Brit. Corros. J., 7 (1972) , 90. [4] Alkire, R. and Nicolaides, G., J. Electrochem Soc., 121 (1974) , 183. [5] Johnson, W. K., Brit. Corros. J., 6 (1971) , 200. [6] Brown, B. F., Fujii, C. T. and Dahlberg, E. P., J. Electrochem. Soc., 116 (1969) , 218. [7] Butler, G., Sttretten, P. and Beynon, J. G., Brit. Corros. J., 7 (1972) , 168. [8] Tsuguo Suzuki, Minoru Yamabe and Yoshiharu Kitamuau, Corrosion, 29 (1973) , 18. [9] 侯文涛,吕明,未发表工作. [10] 中国科学院吉林应用化学研究所金属腐蚀组,金属腐蚀与防护(1976) ,№ 1,p.9. [11] 托马晓夫,H.Д.,金属腐蚀及其保护的理论,华保定等译,中国工业出版社,1964,第7章,第10节. [12] 中国科学院吉林应用化学研究所金属腐蚀简报. [13] Pourbaix, M. J. N., Thermodynamics of Dilute Aqueous Solutions, Edward Arnold & Co., 1949, p. 50, 93. [14] Petersen, J., Werkst. Korros., 28 (1977) , 748. [15] 侯文涛,金属腐蚀与防护(1978) ,№ 1.P |