| CRYSTALLIZATION PROCESS AND DOMAIN STRUCTURE OF AMORPHOUS Gd-Co THIN FILMS |
| Yang Cuiying;Zhou Yuqing;Zhao Jiangao Institute of Physics; Academia Sinica |
|
Cite this article:
Yang Cuiying;Zhou Yuqing;Zhao Jiangao Institute of Physics; Academia Sinica. CRYSTALLIZATION PROCESS AND DOMAIN STRUCTURE OF AMORPHOUS Gd-Co THIN FILMS. Acta Metall Sin, 1979, 15(3): 359-447.
|
|
|
Abstract The crystallization process of Gd_(17)-Co_(83) sputtered thin films has been exami-ned by electron microscopy and electron diffraction. The samples showed a typicalamorphous feature at room temperature and a crystalline state under 550℃. It wasobserved that the crystallization process of Gd_(17)-Co_(83) films underwent a change fr-om an amorphous state through two steps of metastable phase Ⅰ and Ⅱ, and theninto a stable state finally. The metastable phase Ⅱ, however, was not a single ph-ase, but was a mixture of several complex metastable phases. The influence of tem-perature on the domain structure of amorphous Gd-Co thin films has also beenstudied.
|
|
Received: 18 March 1979
|
[1] Vitek, J. M., Vander Sande, J. B. and Grant, N. J., Acta Met., 23 (1975) , 165. [2] Masumoto, T. and Maddin, R., Acta Met., 19 (1971) , 725. [3] Chen, H. S. and Turnbull, D., Acta Met., 17 (1969) , 1021. [4] Peter, Chou, C. P. and Turnbull, D., J. Non-Cryst. Solid, 17 (1975) , 169. [5] Chen, H. S. and Coleman, E., Appl. Phys. Lett., 28 (1976) , 245. [6] Kirchner, H. O. K., Mat. Sci. Eng., 23 (1976) , 95. [7] Herd, S. R. and Chaudhari, P., Phys. Status Solidi, A18 (1973) , 603. [8] 王荫君,陈书潮等,物理学报,26(1977) ,187. [9] Hale, M. E., Fuller, H. W. and Rubinstein, H., J. Appl. Phys., 30 (1959) , 789. [10] 增本健,木村博,日本金属学会志,39(1975) ,273.X |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|