| EFFECTS OF RECRYSTALLIZATION TEXTURES ON THE PLASTIC STRAIN RATIO R AND DEEP-DRAWING PROPERTIES OF COLD ROLLED LOW-CARBON STEEL SHEETS CONTAINING TITANIUM |
| Qiu Li;Zhang Kui;Yin Ying;Liu Yuming;Liu Jianmin Anshan Iron and Steel Company |
|
Cite this article:
Qiu Li;Zhang Kui;Yin Ying;Liu Yuming;Liu Jianmin Anshan Iron and Steel Company. EFFECTS OF RECRYSTALLIZATION TEXTURES ON THE PLASTIC STRAIN RATIO R AND DEEP-DRAWING PROPERTIES OF COLD ROLLED LOW-CARBON STEEL SHEETS CONTAINING TITANIUM. Acta Metall Sin, 1979, 15(4): 462-583.
|
|
|
Abstract The effects of titanium 0.145-0.35% corresponding to the ratio Ti/(C+N)varied from 2.9 to 10.1 on the recrystallization textures of cold rolled low-carbonsteel sheets have been investigated in comparison with the plastic strain ratio Rand deep-drawing properties. For the ratio Ti/(C+N)>4, the main texture com-ponent of (111) [112] is beneficial to the deep-drawing ability; for the ratio Ti/(C+N)<4, that of (100) [011] is detrimental. It would appear that the deep-drawingproperties were substantially determined by the type and degree of the recrystal-lization textures, but not by their erystalline shape. The influence of fine precipi-tates of TiC phase on the recrystallization texture has been discussed.
|
|
Received: 18 April 1979
|
[1] 须藤正俊,铁钢薄板再结晶及集合组织,日本组织基礎共同研究会再结晶部会,1974年,p.99. [2] Shiraiwa, T. and Fujino, N., Proceedings of the 5th International Congress on X-Ray Optics and Microanalysis, Edited by G. Mollenstedt, and Gaukler, K. H., Tubingen, 1968, p. 531. [3] 成田贵一,松本洋,铁钢,58 (1972) ,1330. [4] Vieth, R. W. and Whiteley, R. L., Influence of Crystallographic Orientation on Plastic Anisotropy in Deep Drawing Sheet Steel, Paper Presented at the IDDRG Meeting, June 1964, London. [5] Hu, H., Mechanism of Recrystallization Texture Formation in Deep-Drawing Steels, Paper Presented at the 5th International Congress on Texture, 1978. [6] Evans, P. R. V., Bitcon, J. C. and Hughes, I. F., J. Iron Steel Inst., London, 207 (1969) , 331. [7] Takahashi, M. and Okamoto, A., Effects of Nitrogen Content on Recrystallization Textures of Low-Carbon Steel Sheets, Paper Presented at the 5th International Congress on Texture, 1978. [8] 福田宣雄,清水峰男,塑性加工,13(1972) ,№ 142,841. [9] 松岗孝,高桥政司,铁钢,57(1971) ,1134. [10] Blickwede, D. J., Metal Progr., 95 (1969) , № 4, 87., |