A RAPID METHOD FOR INDEXING THE ELECTRON CHANNELLING PATTERN
Lan Fenlan;Liao Qianchu Central Iron and Steel Research Institute; Ministry of Metallurgical Industry
Cite this article:
Lan Fenlan;Liao Qianchu Central Iron and Steel Research Institute; Ministry of Metallurgical Industry. A RAPID METHOD FOR INDEXING THE ELECTRON CHANNELLING PATTERN. Acta Metall Sin, 1980, 16(1): 104-108.