THE EFFECT OF RARE EARTH MISCHMETAL ON THE TEMPER BRITTLENESS OF TWO LOW ALLOY STEELS CONTAINING MANGANESE AND PHOSPHORUS |
Ji Jingwen;Xiao Lianfang;Gao Huaisun Baotou Institute of Metallurgy |
|
Cite this article:
Ji Jingwen;Xiao Lianfang;Gao Huaisun Baotou Institute of Metallurgy. THE EFFECT OF RARE EARTH MISCHMETAL ON THE TEMPER BRITTLENESS OF TWO LOW ALLOY STEELS CONTAINING MANGANESE AND PHOSPHORUS. Acta Metall Sin, 1980, 16(1): 115-138.
|
|
Received: 18 January 1980
|
[1] Viswanathan, R.. Met. Trans., 2 (1971) , 809. [2] 陈篪,姚蘅,邓枝生,庄韬,邓其源,科学通报,20(1975) ,329.A |