SPATIAL ORIENTATION DISTRIBUTION OF CRYSTALLITES IN COLD-ROLLED AND IN ANNEALED SHEETS OF DEEP-DRAWING PHOSPHORUS STEEL
Hsun Hu U. S. Steel Research Laboratory
Cite this article: 

Hsun Hu U. S. Steel Research Laboratory. SPATIAL ORIENTATION DISTRIBUTION OF CRYSTALLITES IN COLD-ROLLED AND IN ANNEALED SHEETS OF DEEP-DRAWING PHOSPHORUS STEEL. Acta Metall Sin, 1980, 16(2): 121-139.

Download:  PDF(1551KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The cold-rolling and annealing textures of a deep-drawing phosphorus steelhave been studied by he patial orientation distribution of the crystallites. Thecharacteristics of the orientation distribution unctions of the as-cold-rolled andof the annealed sheets were closely examined. The observed features uggest thatthe annealing texture is originated by microband or transition-band nucleation,followed by the rowth of recrystallized grains at the expense of the matrix de-formation textures. The crystallite rientation distribution of the annealed sheetof the deep-drawing phosphorus steel is clearly different from hat of the annealedsheet of deep-drawing aluminum-killed steels.
Received:  18 February 1980     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1980/V16/I2/121

[1] Hu, H., Texture Cryst. Sol., 2 (1976) , 113.
[2] Hu, H., Met. Trans., 8A (1977) , 1567.
[3] Hu, H., Texture Cryst. Sol., 3 (1979) , 215--230.
[4] Hu, H., "Effect of Silicon on Annealing Texture, Plastic Anisotropy, and Mechanical Properties of Low-Carbon Phosphorus-Containing Steels," Proceedings of Symposium on Modern Developments in HSLA Formable Steels, TMS-AIME Fall Meeting, October 24--27, 1977, Chicago, Ⅰ.Ⅱ.
[5] Hu, H., "Low-Carbon Phosphorus Steels for High-Strength Cold-Rolled Sheet Applications," Unpublished work, U. S. Steel Research Laboratory.
[6] Roe, R. J., J. Appl. Phys., 36 (1965) , 2024.
[7] Roe, R. J., J. Appl. Phys., 37 (1966) , 2069.
[8] Bunge, H. J., Z. Metallk., 56 (1965) , 872.
[9] Bunge, H. J., Mathematische Methoden der Texturanalyse, Akademie-Verlag, Berlin, 1969.
[10] Morris, P. R. and Heckler, A. J., Advances in X-Ray Analysis, 1968, Vol. 11, p. 454.
[11] Meieran, E. S., Rev. Sci. Instrum., 33 (1962) , 319.
[12] Lopata, S. L. and Kula, E. B., Trans. AIME, 224 (1962) , 865.
[13] Leber, S., Rev. Sci. Instrum., 36 (1965) , 1747.
[14] Elias, J. A. and Heckler, A. J., Trans. AIME, 239 (1967) , 1237.
[15] Schuiz, L. G., J. Appl. Phys., 20 (1949) , 1030.
[16] Morris, P. R., Texture Cryst. Sol., 2 (1976) , 57.
[17] Jura, J. and Pospiech, J., Texture Cryst. Sol., 2 (1976) , 81.
[18] Bunge, H. J., Tobisch, J. and Mucklich, A., Texture, 1 (1974) , 211.
[19] Humbert, M., Wagner, F. and Baro, R., Texture Cryst. Sol., 3 (1978) , 27.
[20] Davies, G. J., Goodwill, D. J. and Kallend, J. S., J. Appl. Cryst., 4 (1971) , 67.
[21] Hu, H., in Recovery and Recrystallization of Metals, Interscience Publishers, New York, 1963, p. 311. [22] Bunge, H. J., Phys. Status Solidi, 26 (1968) , 167.
[23] Bunge, H. J. and Roberts, W. T., J. Appl., Cryst., 2 (1969) , 116.
[24] Schlafer, D. and Bunge, H. J., Texture, 1 (1974) , 157.
[25] Bunge, H. J., Schleusener, D. and Schlafer, D., Met. Sci. J., 8 (1974) , 413.
[26] Hechler, A. J. and Granzow, W. G., Met. Trans., 1 (1970) , 2089.
[27] Inagaki, H. and Suda, T., Texture, 1 (1973) , 129.
[28] Willis, D. J. and Hatherly, M., in Texture and Properties of Materials, 4th Int. Conf. on Texture, Cambridge, The Metals Society, 1976, p. 48.
No related articles found!
No Suggested Reading articles found!