THERMOGRAVIMETRIC STUDY OF DIRECT CARBURIZING BY NATURAL GAS
Tan Zhicheng;Zhou Lixing;Tan Huiling;Mei Wenlin Dalian Institute of Chemical Physics; Academia Sinica Dept. of Metallurgy; Chongqing University
Cite this article: 

Tan Zhicheng;Zhou Lixing;Tan Huiling;Mei Wenlin Dalian Institute of Chemical Physics; Academia Sinica Dept. of Metallurgy; Chongqing University. THERMOGRAVIMETRIC STUDY OF DIRECT CARBURIZING BY NATURAL GAS. Acta Metall Sin, 1980, 16(2): 239-244.