| IN SITU OBSERVATION OF CRACK NUCLEATION AND PROPAGATION IN a-TITANIUM UNDER TENSILE LOADING BY HVEM |
| Li Yonghong and Tian Fengzuo (Central Nonferrous Metals Research Institute; Ministry of Metallurgical Industry) Li Zongquan; Zhang Lide; Long Qiyi and He Yizhen (Institute of Metal Research; Academia Sinica) |
|
Cite this article:
Li Yonghong and Tian Fengzuo (Central Nonferrous Metals Research Institute; Ministry of Metallurgical Industry) Li Zongquan; Zhang Lide; Long Qiyi and He Yizhen (Institute of Metal Research; Academia Sinica). IN SITU OBSERVATION OF CRACK NUCLEATION AND PROPAGATION IN a-TITANIUM UNDER TENSILE LOADING BY HVEM. Acta Metall Sin, 1981, 17(2): 113-237.
|
|
|
Abstract This paper presents the results obtained from the in situ observations of the crack nucleation and its propagation under tensile loading in HVEM. It was found that some slip bands appeared and slip steps formed at both ends of a slip band through the movement of a great deal dislocations. The crack is initiated at the slip step owing to the stress concentration. Once a crack has nucleated, it will propagate forward under the applied stress. The cracks propagate essentially in two ways: (1) during tensile loading, a large plastic thinning zone is formed near the crack tip. The crack propagates along the thinning zone with a discontinuous manner; (2) the main crack propagates by a mechanism of coalescence of microcracks in the vicinity of the crack tip. Additionally, it was noticed that the grain boundary is not probably the preferential sites of the crack nucleation and propagation in α-titanium.
|
|
Received: 18 February 1981
|
[1] Drucker, D. C. and Gilman, J. J., Fracture of Solids, Vol. 20, Interscience Pub., 1962, p. 393. [2] Imura, T., Yukawa, N., Saka, H., Nohara, A., Noda, K. and Ishikawa, I., in High Voltage Electron Microscopy, Proc. Third Inter. Conf., eds. P. R. Swann et al., Academic Press, London and New York, 1974, p, 199. [3] Campany, R. G., Smallman, R. E. and Loretto, M. H., Metal Sci. 10 (1976) , 261. [4] Bauer, R. W., Geiss, R. H., Lyles, R.L. and Wilsdorf, H. G. F in Electron Microscopy and Structure of Materials, G.Thomas, Univ. California Press, Berkeley, Los Angeles, London,1972, p. 85. [5] Fujita, H. and Yamada, H., J. Phys. Soc. Jap.,29(1970) , 132. [6] Lyles, R. L., Jr., and Wilsdorf, H. G. F., Acta Met., 23 (1975) , 269 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|