Please wait a minute...
Acta Metall Sin  1981, Vol. 17 Issue (2): 161-167    DOI:
Current Issue | Archive | Adv Search |
VACUUM VAPORIZATION OF CERTAIN ELEMENTS IN CARBON-SATURATED IRON MELT
Liu Shuzhen (Research Institute of Wuhan Iron and Steel Company)
Cite this article: 

Liu Shuzhen (Research Institute of Wuhan Iron and Steel Company). VACUUM VAPORIZATION OF CERTAIN ELEMENTS IN CARBON-SATURATED IRON MELT. Acta Metall Sin, 1981, 17(2): 161-167.

Download:  PDF(555KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The behaviour of vaporization of S, Mn, Cu, Si and P in the carbonsaturated iron melt has been investigated with respect to the effects of smelting time and temperature, as well as pressure in vacuum chamber and specific surface area of melt in a vacuum induction furnace. It was shown that an arrangement in vaporizability order of these elements may be properly put and a maximum rate of vaporization for S, Mn and Cu occurs at 1330℃.
Received:  18 February 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I2/161

[1] Oleette, M., Physical Chemistry of Process Metallurgy, Pt 2, Met. Soc. Conf. 1959, Vol. 8, p. 1065-1087.
[2] Ward, R. G., J. Iron Steel Inst. 201 (1963) , 11.
[3] Fischer, W. A. und Hoffmann, A., Arch Eisenhuettenw., 29 (1958) , 339.
[4] BISRA, Steel Times, 188 (1964) , 347.
[5] Wever, F., Fischer, W. A. und Engelbrecht, H., Stahl Eisen, 74 (1954) , 1515.
[6] Fischer, W. A., Arch Eisenhuettenw., 31 (1960) , 1.
[7] Ardenne, M., Schiller. S., Kuntscher, W., Thiel, H. und Meyer, L., Neue Huett, 6 (1961) , 198.
[8] Bungardt, K. und Sychrovsky, H., Stahl Eisen, 76 (1956) , 1040.
[9] Gill, G. M., Ineson, E. and Austin, G. W., J. Iron SteeL Inst, 191 (1959) , 172.
[10] 韩耀文,金属学报,6(1963) ,98.
[11] Fischer, W. A., Janke, D., Metallurgische Elektrochemie, Springer-Verlag, Berlin, 1975, p. 204, 244.
[12] 鈴木楨一、伊逹山静男、工藤武司,鉄鋼,49(1963) ,465.
[13] 邵象华,金属学报,7(1964) ,85.
[14] King, T. B., Vacuum Metallurgy, ed. R. F. Bunshah, Chapman & Hall, London, 1958, p. 35.
[15] Ogino, Y., Trans. Iron Steel Inst. Jap., 14 (1974) , 82.
[16] #1
No related articles found!