Please wait a minute...
Acta Metall Sin  1981, Vol. 17 Issue (4): 374-385    DOI:
Current Issue | Archive | Adv Search |
LATTICE DEFECTS IN SOLID HELIUM
by Hideji Suzuki (Department of Physics; Faculty of Science; University of Tokyo; Japan)
Cite this article: 

by Hideji Suzuki (Department of Physics; Faculty of Science; University of Tokyo; Japan). LATTICE DEFECTS IN SOLID HELIUM. Acta Metall Sin, 1981, 17(4): 374-385.

Download:  PDF(822KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Brief historical details concerning the defects of solid helium are reviewed.The plastic deformation in hop ~4He, anomalous temperature dependence of the sound velocity and the force for the steady creep in ~4He and bcc ~3He are discussed.
Received:  18 April 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I4/374

[1] Huzuki, H., J. Phys. Soc. Jpn., 35 (1973) , 1472.
[2] Suzuki, H,, J. Phys. Soc. Jpn., 42 (1977) , 1865.
[3] Sakai, A., Nishioka, Y. and Suzuki, H., J. Phys. Soc. Jpn., to be published.
[4] 铃木秀次,固体物理13(1970) ,231.
[5] Wanner, R., Iwasa, I. and Wales, S., Solid State Commun., 18 (1976) , 853.
[6] Iwasa, I., Araki, K. and Suzuki, H., Proc. 6th Int. Conf. Internal Friction and Ultrasonic Attenuation in Solids (Univ. Tokyo Press, Tokyo, 1977) p. 549; J. Phys. Soc. Jpn. to be published.
[7] Andreev, A., Keshishev, K., Mezhov-Deglin, L. and Shal, Nikov, A., ZhETF Pis. 9 (1969) , 507. Translation: JETP Letters, 9 (1969) , 306.
[8] Alexander, Ho and Haasen, P., Solid State Phys., 22 (1968) , 110.
[9] Granato, A. V. and Lucke, K, J. Appl. Phys., 27 (1956) , 583.
[10] Ninomiya, T., J. Phys. Soc. Jpn., 36 (1974) , 399.
[11] Taylor, G. I., J. Inst. Met., 62 (1938) , 307.
[12] Suzuki, H., Dislocation Dynamics, Ed. by A. R. Rosenfield, et al., McGraw-Hill, New York, 1968, p. 679."
No related articles found!
No Suggested Reading articles found!