STUDIES OF CARBIDES IN 6Cr4Mo3Ni2WV STEEL
by Liu Wenxi; Wang Binghui; Chong Keduan and Zhang Cunxin
Cite this article: 

by Liu Wenxi; Wang Binghui; Chong Keduan and Zhang Cunxin. STUDIES OF CARBIDES IN 6Cr4Mo3Ni2WV STEEL. Acta Metall Sin, 1981, 17(5): 513-600.

Download:  PDF(4663KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The carbides in 6Cr4Mo3Ni2WV steel have been studied by TEM, electrolytic extraction phase analysis, X-ray diffraction and EMPA. It was confirmed that the M_2C with long-range ordered carbon distribution and V_4C_3 with short-range ordered vacancy distribution are present in the residual carbides of the steel quenched from 1120℃. The nucleation of V_4C_3 with concomitant M_2C was observed during the tempering precipitation.The distribution of alloying elements partitioned between steel matrix and carbides is thus ascertained.
Received:  18 May 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I5/513

[1] Kuo, K., J. Iron Steel Inst., 173 (1953) , 363.
[2] Shaw, S. W. K. and Quarrell. A. G., J. Iron Steel Inst., 185 (1957) , 10.
[3] Irvine, K. J., Growe, D. J. and Picketing, F. B., J. Iron Steel Inst., 195 (1960) , 386.
[4] Raynor, D., Whiteman, J. A. and Honeycombe, R. W. K., J. Iron Steel Inst., 204 (1966) , 1114.
[5] Honeycombe, R. W. K., Structure and Strength of Alloy Steels, Climax Molybdenum Co., London, p, 1.
[6] 上海钢铁研究所,未发表资料,1978.
[7] Steven, G., Hauser, J. J., Neumeyer, T. A. and Capenos, J. M., ASM Trans. Q., 62 (1969) , 180.
[8] Bridge, J. E., Maniar, G. N. and Philip, T. V., Metall. Trans., 2 (1971) , 2209.
[9] Parthe, E. and Sadagopan, V., Acta Cryst., 16 (1963) , 202.
[10] 桶谷繁雄,電子線回圻金属炭化物研究,東京,1971,p.202.
[11] Billingham, J., Bell, P. S. and Lewis, M. H., Acta Cryst., A28 (1972) , 602.
[12] Sauvage, M. and Parthe, E., Acta Cryst., A28 (1972) , 607.
[13] 郭可信,金属学报,2(1957) ,303.
[14] H. M.,钢的碳化物分析,机械工业出版社,北京,1959,p.13.
[15] #12
[16] Dyson, D. J. and Keown, S. R., Acta Metall., 14 (1966) , 867.
[17] Baker, R, G. and Nutting, J., Iron Steel Inst., London, Spec. Rep., №. 64, 1959. , p. 1,
[18] 俞学节,金属学报,16(1980) ,53.T
No related articles found!
No Suggested Reading articles found!