IDEAL ECP MAPS FOR DIFFERENT CUBIC CRYSTALS AND THEIR RAPID INDEXING METHOD |
by Liao Qianchu and Lan Fenlan (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry) |
|
Cite this article:
by Liao Qianchu and Lan Fenlan (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry). IDEAL ECP MAPS FOR DIFFERENT CUBIC CRYSTALS AND THEIR RAPID INDEXING METHOD. Acta Metall Sin, 1981, 17(5): 565-577.
|
Abstract A set of ideal ECP maps for different cubic crystals was theoretically delineated by using the sterographical projection method of crystal planes. The data given by the maps are tabulated as a new convenient chart for rapidly indexing the ECP of cubic crystals experimentally obtained. This method saved wasting time from the indexing already. The error analysis shows that the present indexing method seems to be available to the cases of the zone axis both parallel and inclined to the optical axis of SEM.
|
Received: 18 May 1981
|
[1] Van Essen, C. G., Schulson, E. M. and Donashay, R. H., Nature, 225 (1970) , 847; J. Mater. Sci., 6 (1971) , 213. [2] Schulson, E. M., J. Sci. Instrum., 2 (1969) , 361; J. Appl. Phys., 42 (1971) , 3894. [3] Newburg, D. E. and Jop. D. C., Proc. 25th Anniversary Meeting of EMAG, Cambridge, 1971, p. 306. [4] 蓝芬兰,廖乾初,金属学报,16(1980) ,104.Q |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|