YIELD STRENGTH OF METALS AND ALLOYS
by Hideji Suzuki (Department of Physics; Faculty of Science; University of Tokyo; Japan)
Cite this article: 

by Hideji Suzuki (Department of Physics; Faculty of Science; University of Tokyo; Japan). YIELD STRENGTH OF METALS AND ALLOYS. Acta Metall Sin, 1981, 17(5): 583-594.

Download:  PDF(811KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A review covering the present state of yield strength of metals and alloys is presented. Emphasis is placed on slip and dislocation, multiplication of dislocations, plastic flow rate equation, Peierls stress, temperature dependence of the yield stress and effect of solute atoms.
Received:  18 May 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I5/583

[1] Suzuki, H., Strength of Metals (AGNE, Tokyo, 1972) .
[2] Frank, F, C. and Read, W. T., Phys. Rev., 79 (1950) , 722.
[3] Washburn, J., Groves, G. W., Kelly, A. and Williamson G. K., Phil. Mag., 5 (1960) , 991.
[4] Dash, W. C., Dislocations and Mechnical Properties of Crystals Ed. Fisher, J. C. et al., John Wiley and Sons, New York, 1957, p. 57.
[5] Wilsdorf, H. G. F., Structure and Properties of Thin Films, Ed. by C. A. Neugebauer et al., John Wiley and Sons, New York, 1959, p. 151.
[6] Nemoto, M. and Koda, S., Jpn. J. Appl. Phys., 4 (1965) , 583.
[7] Furubayashi, E., J. Phys. Soc. Jpn., 27 (1969) , 130.
[8] Jotmston, W. G. and Gilman, J. J., J. Appl. Phys., 30 (1959) , 129.
[9] Suzukl H. and Kuramoto, E., Proc. Int. Conf. Strength of Metals and Alloys, Trans. Jpn. Inst. Metals, 9 (1968) , Suppl., p. 697.
[10] Peierls, R., Proc. Phys. Soc., 52 (1940) , 34.
[11] Nabarro, F. R. N., Proc. Phys. Soc., 59 (1947) , 256.
[12] Huntington, H. B., Proc. Phys. Soc., 68 (1955) , 1043.
[13] Kuhlmann-Wilsdorf. D., Phys. Rev., 120 (1960) , 773.
[14] Suzuki, H., Dislocation Dynamics, Ed. by A. R. Rosenfield et al., McGraw-Hill, New York, 1968, p. 679.
[15] Basinik, Z. S., Kuramoto, E. and Takeuchi. S., Phys. Status Solidi, (a) 22 (1974) , 81.
[16] Minami, F., Kuramoto, E. and Takeuchi, S., Phys. Status Solidi, (a) 22 (1974) , 81.
[17] Cell, V., Kabler, M., Ninomiya, T. and Thomson, R., Phys. Rev., 131 (1963) , 58.
[18] Dorn, J. E. and Rajnak, S., Trans. Metall. Soc. AIME, 230 (1964) 1052.
[19] Conte, R., Groh, P. and Escaig, B., Phys. Status Solidi, 28 (1968) , 475.
[20] Suzuki, H., Machrichten der Akademie der Wissenshaften in Gottingen II, Mathematisch-Physikalisch Klasse Nr. 6, 1971, S. 113.
[21] Suzuki, H., Rate Processes in Plastic Deformation of Materials Ed. by J. C. M. Li and A.K. Mukherjee, ASM, Cleveland, 1975, p. 47.
[22] Suzuki, H., Dislocations in Solids, Ed. by F. R. N. Nabarro, North-Holland, Amsterdam, 1978.
[23] Takeuchi, S., Yoshida, H. and Taoka, T., Proc. Int. Conf. Strength of Metals and Alloys, Trans. Jpn. Inst. Metals. 9 (1968) , Suppl. p. 715.
[24] Takeuchi, S., Furubayashi, E. and Taoka, T., Acta Metall., 15 (1967) , 1179.
[25] Takeuchi, S., .L Phys. Soc. Jpn., 27 (1969) ,929.
No related articles found!
No Suggested Reading articles found!