ON THE STEADY STATE CREEP OF ALLOY Ti-679
Cao Mingzhou; Zhao Jixiang; Su Ge and Wan Xiaojing
Cite this article: 

Cao Mingzhou; Zhao Jixiang; Su Ge and Wan Xiaojing. ON THE STEADY STATE CREEP OF ALLOY Ti-679. Acta Metall Sin, 1981, 17(6): 690-694.

Download:  PDF(363KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The steady state creep rate of alloy Ti-679 under various temperatures and stresses was examined. A cyclic test on strain rate was also made of its apparent activated area as a function of temperature. Some approaches to the creep mechanism of the alloy are discussed.
Received:  18 June 1981     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1981/V17/I6/690

[1] Conarad, H., Demeester, B., Yin, C. and Doner. M., Rate Processes in Plastic Deformation of Materials, Ed. By Li, J. C. M. and Mukheriee, A. K., Cleveland, 1975, p. 175.
[2] Surek, T., Kuon, L. G., Luton, M. J. and Jonas, J. J., Rate Processes in Plastic Deformation of Materials, Ed. by J. C. M. Li and A. K. Mukherijee, Cleveland, 1975, p. 629.
[3] Paton, N. E. and Mahoney, M. W., Metall. Trans., 7A (1976) , 1685.
[4] Conrad, H., Doner, M. and Demesster, B., Titanium Science and Technology, Ed. by R. I. Jaffee, and H. M. Burte, Plenum, New York, 1973, p. 969.
[5] Conrad, H. and Jones, R., The Science, Technology and AppLication of Titanium, Ed. by R. I. Jaffee and N. E. Promisel, Pergamon, Oxford, 1970.
[6] Winstone, M. R., Rawlings, Rees D. and West, D. R. F., J. Less-Common Met., 39 (1975) , 205.
[7] Kohoe, M. and Brromfield, R. W., Titanium Science and Technology, Ed. by R. I. Jaffee and H. M. Butte, Plenum, New York, 1973, p. 2167.
[8] Rosen, A. A. and Rotten, A., Mater. Sci. Eng., 22 (1976) , 23.8
No related articles found!
No Suggested Reading articles found!