Please wait a minute...
Acta Metall Sin  1982, Vol. 18 Issue (1): 38-125    DOI:
Current Issue | Archive | Adv Search |
EFFECT OF THE MODE OF OVERLOAD ON THE BEHAVIOUR OF FATIGUE CRACK PROPAGATION
Ouyang Jie; Yan Minggao (Institute of Aeronautical Materials; Beijing)
Cite this article: 

Ouyang Jie; Yan Minggao (Institute of Aeronautical Materials; Beijing). EFFECT OF THE MODE OF OVERLOAD ON THE BEHAVIOUR OF FATIGUE CRACK PROPAGATION. Acta Metall Sin, 1982, 18(1): 38-125.

Download:  PDF(2999KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effects of different modes of overload, including tensile, compressive, tensile-compressive and compressive-tensile, on the behaviour of fatigue crack propagation in LY12 A1 alloy were investigated. From a study of the changes in micro-morphology, the plastic zone size and strain distribution around the crack tip and the fracture analysis before and after various overloading, it is suggested that various modes of overload produce different influences on FCP, and the retardation behaviour of FCP after tensile overloading may be described as a combination effect of several factors acting on the crack tip and its surrounding region. A general mechanism of the effect of tensile overload on FCP behaviour is proposed.
Received:  18 January 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I1/38

1 Hudson, C. M.; Hardrath, H. F.; NASA TN-D-960, 1961.
2 Von Euw, E. F. J.; Hertzberg, R. W.; Roberts, R., Am. Soc. Test. Mater., Spec. Tech. Publ. No 513, 1972, p. 230.
3 Hsu, T, M.; Lassiter, L. W., AIAA Paper No 74-365, 1974.
4 顾明达;张诗捷;颜鸣皋,HKCL Tech.Rep.,79-2-2,1979.
5 Chanani, G. R., Met. Eng. Q., 15 (1975) , No 1, 40.
6 Christensen, R. H., Metal Fatigue, McGraw-Hill, New York, 1959, p. 385.
7 Schijve, J.; Brock, D., Aircr. Eng., 34 (1962) , 314.
8 平修二;田中啓介;山崎利春,材料,27(1978) ,251.
9 Elber, W., Am. Soc. Test. Mater., Spec. Tech. Publ.,No 486, 1971, p. 230.
10 Schijve, J., Eng. Fract. Mech., 11 (1979) , 182.
11 黄王璞,未发表工作,1976.
12 Schijve, J., Am. Soc. Test. Mater., Spec. Tech. Publ., No 595, 1976, p. 3.
13 Oppel, G. U.; Hill, P. W., Exp. Mech., 4 (1964) , No 7, 206.
14 Lachenbruch, A.H., J. Geophys. Res., 66 (1961) , 4273.
15 Forman, R. G.;Kearney, V. E.; Engle, R. M., Trans. ASME, Ser. D: J. Basic Eng., 89 (1967) , 459.
No related articles found!