Please wait a minute...
Acta Metall Sin  1982, Vol. 18 Issue (2): 176-186    DOI:
Current Issue | Archive | Adv Search |
DETERMINATION OF EQUILIBRIUM CONSTANT OF Ce-O OR Nd-O IN LIQUID IRON
Han Qiyong;Liu Shiwei;Niu Hongbing;Tang Zhiwei Beijing University of Iron and Steel Technology
Cite this article: 

Han Qiyong;Liu Shiwei;Niu Hongbing;Tang Zhiwei Beijing University of Iron and Steel Technology. DETERMINATION OF EQUILIBRIUM CONSTANT OF Ce-O OR Nd-O IN LIQUID IRON. Acta Metall Sin, 1982, 18(2): 176-186.

Download:  PDF(1207KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Autoradiographs have shown that there is an obvious reaction between Ce and Nd in liquid iron and MgO,CaO crucible wall.For reaching the Ce-O, Nd-O equilibrium,a long smelting period and the adding of rare earth elements in several batches were needed to ensure the full reaction between the rare earth elements in melt and the crucible wall.The dissolved Ce or Nd content in iron was measured by means of radioactive isotopes ~(141)Ce or ~(147)Nd together with electrolysis in the organic electrolyte of samples.The oxygen activity was measured by solid electrolyte sensors made of ZrO_2(MgO) tube. Ce_2O_(3(s))=2[Ce]+3[O] △G*_(Ce_2O_3)=451150-161.68T lgK_(Ce_2O_3)=-(98611)/T+35.34 Nd_2O_3=2[Nd]+3[O] △G*_(Nd_2O_3)=375010-123.7T lgK_(Nd_2O_3)=-(81970)/T+27.04 The standard free energy of dissolution of Nd in liquid iron: Nd_(1)=[Nd]1% △G=19790-30.40T lgγ*_(Nd)=(4326.1)/T-4.154.
Received:  18 February 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I2/176

1#12
2 Hitchon,J.W.F.;Chaillou,A.;Olette,M.,Report IRSID(1966) ,Cerium and Lanthanum as Deoxidizers and Desulfurizers in Liquid Iron.
3 Fischer,W.A.;Bertram.H.,Arch.Eisenhuettenwes.,44(1973) ,87,97.
4 石川遵平;井上博文;三本木贡治,东北大学选鉱制炼研究所,29(1973) ,193.
5 Elgammal,T.;Dehl,W.;Lorenz,L.,Proceedings of the 4th International Conference on Vacuum Metallurgy,Tokyo,1973,Iron Steel Inst,Jpn.,Tokyo 1974,Sect.2,p.125.
6 Janke,D.;Fischer,W.A.,Arch Eisenhuettenwes:,49(1978) ,425.
7 王常珍;王福珍;杜英敏;张小平,金属学报,16(1980) ,1,83.
8#12
9 Vahed,A.;Kay,D.A.R.,Metall.Trans.,7B(1976) ,375.
10 Fruehan,R.J.,Metall.Trans.,5(1974) ,345.
11 北京钢铁学院物化教研室同位素教研组,金属学报,13(1977) ,202.
12 韩其勇;方克明;吴卫江等,单一稀土夹杂的组成与形态(待发表).
13 Janke,D.;Fischer,W,A.,Arch.Eisenhuettenwes.,48(1977) ,311.
14 韩其勇;吴卫江;方克明;霍成章;周小龙,中日钢铁学术会议,第一届炼钢学术会议会议报告,北京,1981,p.25.
15 Janke,D.;Fischer,W.A.,Arch.Eisenhuettenwes.,46(1975) ,755.
16 Janke,D.;Fischer,W.A.,Arch.Eisenhuettenwes.,47(1976) ,195.
17 Gschneidner,K.A.;Kippenhan,N.;McMaster,O.D.,Thermochemistry of the Rare Earths,Report № IS-RIC-6,Rare Earth Information Center,Amesl Iowa,1973.
18 Elliott,J.F.,Electr.Furnace Proc.,32(1974) ,62.
19 沢村宏,钢铁化学热力学,诚文堂新光社,1972,附表 p.43.
20 Ejima,A.;Suzuki,K.-I.;Harada,N.;Sanbongi,K.,Trans.Iron Steel Inst.Jpn.,17(1977) ,349.
No related articles found!