THERMODYNAMICAL STUDY ON SOLVENT EXTRACTION OF METALS
Teng Teng;Li Yigui;Cheng Zhenhua;Zhang Lianping Department of Chemistry and Chemical Engineering; Tsinghua University; Beijing
Cite this article: 

Teng Teng;Li Yigui;Cheng Zhenhua;Zhang Lianping Department of Chemistry and Chemical Engineering; Tsinghua University; Beijing. THERMODYNAMICAL STUDY ON SOLVENT EXTRACTION OF METALS. Acta Metall Sin, 1982, 18(2): 201-210.

Download:  PDF(760KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the solution theory,the thermodynamical approaches to calculation of the component activity coefficients in organic phases,to determination of the thermodynamical equilibrium constant of metal extraction reaction and to predic- tion of the metal extraction equilibrium distribution are presented.Three neutral solvent-metal extraction systems,TBP-UO_2Cl_2,TBP-UO_2(NO_3)_2 and (C_7H_(15))_2SO-UO_2 (NO_3)_2,have been tested solely by thermodynamical method.Seven models have also been examined and compared,Among them,the Scatchard-Hildebrand and Guggenheim ones are more simple and convenient for calculating practice.These two models have tried all available to both quarternary and ternary organic phases.
Received:  18 February 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I2/201

1 Davis,W.;Mrocheck,J.,Jr.;Judkins,R.R.,J.Inorg.Nucl.Chem.,32(1970) ,1689.
2 Watson,S.B.;Rainey,R.H.,DRNL-TM-5123,1975.
3 Homer,D.E.,ORNL-TM-2711,1970,p.27.
4 Goldberg,S.M.;Benedict,M.,Nucl.Sci Eng.,47(1972) ,169.
5 #12
6 李以圭;滕藤;张良平,清华大学学报,20(1980) ,№3,7.
7 #12
8 #12
9#12
10#12
11 Irving,H.M.N.H.,Ion Exchange and Solvent Extraction,Vol.6,Ed.Marinsky,J.A.;Marcus,Y.,Marcel Dekker,New York,1974,p.139.
12 Wingefors,S.;Liljenjin,J.O.;Saalman,E.,International Solvent Extraction Conference-80,Liege,Vol.3,1980,Report № 80-116,Association of Engineers of Univ.of Liege,Belgium.
13 Kertes,A.S.;Grauer,F.,J.Phys.Chem.,77(1973) ,3107.
14 Tsimering,L.;Kertes,A.S.,International Solvent Extraction Conference-74,Lyon,Vol.1,(1974) ,Soc.Chem.Ind.,London,p.1433.
15 Kertes,A.S.;Tsimering,L.,J.Phys.Chem.,81(1977) ,120.t
No related articles found!
No Suggested Reading articles found!