PRECIPITATION OF γ′-PHASE AND CONTROLLED HEAT TREATMENT OF IRON-NICKEL-BASE SUPERALLOYS
Yang Qibin Zhang Yongchang Sun Guifen Shi Changxu (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 9 September; 1980; Revised manuscript 8 October; 1981)
Cite this article: 

Yang Qibin Zhang Yongchang Sun Guifen Shi Changxu (Institute of Metal Research; Academia Sinica; Shenyang) (Manuscript received 9 September; 1980; Revised manuscript 8 October; 1981). PRECIPITATION OF γ′-PHASE AND CONTROLLED HEAT TREATMENT OF IRON-NICKEL-BASE SUPERALLOYS. Acta Metall Sin, 1982, 18(4): 387-394.

Download:  PDF(1076KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The study has demonstrated that the improvement of yield strength of iron-nickel-base superalloys was markedly performed by adjusting the cooling rate in the course of aging, e.g. the increase of yield strength of IA alloy uprises to 13-17 kgf/mm~2, or the relative increment of 20-25%, provided by furnace cooling instead of air cooling. Its grain boundaries are changed and the notch sensitivity is remedied. The results showed that this improvement is mainly due to full precipitation of γ'-phase. Thus, it seems to be confirmed that an adoption of the logarithm furnace cooling may both increase the vield strength and shorten the time of heat treatment, hence, the consumption of energy and manpower can be saved as well.
Received:  18 April 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I4/387

1 郭建亭;朱耀霄;师昌绪,金属学报,10(1974) ,74.
2 Brown, J.T.; Bulina, J., High Temperature Materials, Eds. Hehemann, R.F.; Ault, G.M., Wiley New York,1957, p.38.
3 Joseph, G.; Mumau, R.R., NASA SP-5106,(1972) , p.24-40.
4 上海第五钢铁厂中心试验室,国外金属材料选编(Inconel 718合金专辑),№ 11,1977,p.108.
5 Moll, J.H.; Maniar, G.N.; Muzyka, D.R., Metall. Trans.,2(1971) ,2153. 6 Eichelberger, T.W., Trans. ASM,50(1958) ,738.
7 金属研究所技术资料,GH135铁基高温合金汇编,1974,p.78,109,图IV-8.
No related articles found!
No Suggested Reading articles found!