Acta Metall Sin  1982, Vol. 18 Issue (5): 534-539    DOI:
Current Issue | Archive | Adv Search |
METASTABLE EXTENSION OF SOLID SOLUBILITY OF CERTAIN SIMPLE METALS OR METALLOIDS IN Ag
Zhou Xinming; Jin Jialu; Ning Yuantao; Zhao Zhongmin (Institute of Precious Metals Research; Kunming)
Cite this article: 

Zhou Xinming; Jin Jialu; Ning Yuantao; Zhao Zhongmin (Institute of Precious Metals Research; Kunming). METASTABLE EXTENSION OF SOLID SOLUBILITY OF CERTAIN SIMPLE METALS OR METALLOIDS IN Ag. Acta Metall Sin, 1982, 18(5): 534-539.

Download:  PDF(512KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The metastable extension of solid solubility of certain simple metals or metalloids in Ag has been studied by means of the lattice parameters measurement when the aUoy specimens quenched from melts. It is found that the solid solubility metastable extension of such elements in Ag that form a lot of peritectic binary alloys with Ag is conformed to the rule of valence electron concentration, but that of those which form eutectic or monotectic alloys does not satisfy the rule. The peritectic alloys may be classified into two types with quite different behaviours of solid solubility metastable extension. It seems to be easily clarified that the influence of the composition range of intermediate phase on the solid solubility metastable extension is more important than its stability. The reason why Si is less soluble in Ag has been also discussed by Miedema's theory.
Received:  18 May 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I5/534

1 Hansen, M.; Anderko, K., Constitution of Binary Alloys, McGraw-Hill, New York, 1958, p. 1-57.
2 Elliot, R. P., Constitution of Binary Alloys, First Supplement, McGraw-Hill, New York, 1965, 1-22.
3 Pearson, W. B., A Handbook of Lattice Spacings and Structure of Metals and Alloys, Pergamon Press, London, 1958, p. 259-308.
4 Anantharaman, T. R.; Romachandrarao, P.; Suryanarayana, C.; Lele, S.; Chattopadnyay, K., Trans. Indian Inst. Met., 30 (1977) , 425.
5 Duwez, P., ASM Trans Q., 60 (1967) , 607.
6 Anantharaman, T. R.; Suryanarayana, C., J. Mater. Sci., 6 (1971) , 1111.
7 Klement, W., Jr.; Luo, M. L., Trans Metall. Soc. AIME, 227 (1963) , 1253.
8 Miedema, A. R.; Boom, R.; de Boor, F. R., J. Less-Common Met., 41 (1975) , 283.
9 Miedema, A. R., ibid., 46 (1976) , 67.