Please wait a minute...
Acta Metall Sin  1982, Vol. 18 Issue (5): 550-642    DOI:
Current Issue | Archive | Adv Search |
TENSILE DEFORMATION BEHAVIOUR OF CARBON STEEL UNDER MEDIUM-HIGH TEMPERATURE
Luo Xiyu (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing); Imamura Jun (Fundamental Research Laboraties; Nippon Steel Corporation; Japan)
Cite this article: 

Luo Xiyu (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing); Imamura Jun (Fundamental Research Laboraties; Nippon Steel Corporation; Japan). TENSILE DEFORMATION BEHAVIOUR OF CARBON STEEL UNDER MEDIUM-HIGH TEMPERATURE. Acta Metall Sin, 1982, 18(5): 550-642.

Download:  PDF(4295KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A systematical study was made of the tensile deformation behaviour of 4 different carbon steels, containing 0.10, 0.25, 0.39 and 0.71% C respectively, with initial austenite grain size 800μm under temperature 700—1300℃ at the strain rate 6.7×10~(-4)—6.7×10~(-2)S~(-1). It was indicated that the equation of deformation in the region of austenite phase controlled by the heat activation process is quite agreed with (?)=Aσ_M~nexp(-Q/RT) and the maximum deformation stress is decreased with the increasing of their C content. In the binary phase α+γ region, an embrittlement appears under temperature slightly lower than A_3 point and may become more or less to toughen as the increase of the C content.
Received:  18 May 1982     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1982/V18/I5/550

1 田村今男,日本金属学会会报,16(1977) ,877.
2 铃木洋夫;山口重裕,日本铁钢基礎共同研究会,高温变形部会,1979,p.113.
3 Nakamura, T.; Uekl, M., Trans Iron Steel Inst Jpn., 15 (1975) , 185.
4 Wray, P. J.; Holmes, M. F., Metall. Trans., 6A (1975) , 1189.
5 Wray, P. J., Metall. Trans., 6A (1975) , 1197.
6 作井诚太;酒井拓;村濑曄夫,日本金属学会誌,39(1975) ,535.
7 作井诚太;酒井拓;沢田裕冶,日本金属学会誌,40(1976) ,1284.
8 作井诚太;酒井拓;武石和夫,铁钢,62(1976) ,856.
9 作井诚太;酒井拓;ibid.,63(1977) ,285.
10 铃木洋夫;中村泰,日本金属学会会报,18(1979) ,748.
11 铃木洋夫;西村哲;山口重裕,铁钢,65(1979) ,2038.
12 铃木洋夫;西村哲;今村淳,中村泰,ibid.,67(1981) ,1180.
13 Mintz, B.; Arrowsmith, J. M., Met. Technol., 6 (1979) , 25.
14 山中和夫;寺崎富久长;大谷泰夫;小田光雄;吉原正裕,铁钢,65(1979) ,1410.
15 酒井拓,日本金属学会会报,17(1978) ,195.
16 Mead, H. W.; Birehenall, C. E., J. Met., 8 (1956) , 1336.
17 今村淳;铃木洋夫;宫崎武志,铁钢,66(1980) ,s804.
No related articles found!