Please wait a minute...
Acta Metall Sin  1983, Vol. 19 Issue (1): 53-58    DOI:
Current Issue | Archive | Adv Search |
RESISTIVITY ANOMALY IN METALLIC GLASSES(Fe_(1-x)Co_x)_(78)Si_(9.5)B_(12.5)
GUO Huiqun; SHEN Baogen; ZHAN Wenshan; PAN Xiaoshuo(Institute of Physics; Academia Sinica; Beijing)
Cite this article: 

GUO Huiqun; SHEN Baogen; ZHAN Wenshan; PAN Xiaoshuo(Institute of Physics; Academia Sinica; Beijing). RESISTIVITY ANOMALY IN METALLIC GLASSES(Fe_(1-x)Co_x)_(78)Si_(9.5)B_(12.5). Acta Metall Sin, 1983, 19(1): 53-58.

Download:  PDF(463KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The electrical resistivity measurements of the amorphous (Fe_(1-x)Co_x)_(78)Si_(9.5)B_(12.5)(x=0—1.0) alloys were made by a fourprobe technique at temperature range from 4.2 to 300K. It was found that the resistivity minima have been observed over the whole concentration range for x=0—1.0. The temperature T_(min) at which the resistivity is minimum increased with increaing Co content, and approached to the maximum at x=0.9. Below T_(min) the resistivity can be described by a logarithmic temperature dependence over the whole content. In the temperature range between T_(min) and 100K the resistivity has a T~2 temperature dependence and follows T_(3/2) temperature dependence above 100K. In summary, the temperature dependence of the electrical resistivity for all content may be expressed at temperature range (9.5—100K) by ρ/ρ_(min)=ρ_0+AlnT+BT~2. A Kondo-type resistivity minimum has been observed in these alloys, A T~2 temperature dependence of resistivity may originate from electron-phonon scattering.
Received:  18 January 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I1/53

1 Hasegawa, R.; Tsuei, C. C., Phys. Rev. B, 2(1970) , 1631.
2 Hasegawa, R.; Tsuei, C. C., Phys. Rev. B, 3(1971) , 214.
3 Babic, E.; Marohnic, Z.; Ivkov, J., Solid state Commun., 27(1978) , 441.
4 Rapp, o.; Bhagat, S. M.; Johannesson, Ch., ibid., 21(1977) , 83.
5 Tsuei, C. C., Anorphous Magnetism Ⅱ, Proc. of the 2nd Int. Symposium on Amorphous Magnetism, Eds. Levy, R. A.; Hasegawa, R., Plenum Press, New York, 1977, p. 181.
6 Cochrane, R. W.; Harris, R.; Stroem-Olson, J.O.; Zuckermann, M.J., Phys. Rev. Lett., 35(1975) , 676.
7 詹文山;沈保根;郭慧群,待发表.
8 Rao, K. V.; Gudmundsson, H.; Astroem, H. U., J. Appl. Phys., 50(1979) , 1592.
9 Rayne, J. A.; Levy, R. A., Amorphous Magnetism Ⅱ, Proe. of the 2nd Int. Symp. on Amorphous Magnetism, Eds. Levy, R. A.; Hasegawa, R., Plenum Press, New York, 1977, p.319.
10 Tsuei, C. C.; Lilienthal, H., Phys. Rev. B, 13(1976) , 4899.
11 Fujimori, H.; Kikuchi, M.; Obi, Y.; Mosumoto, T., Sci. Repts Res. Inst., Tohaku Univ., A26(1976) , 36.
12 郭慧群;沈保根;俞伯良;詹文山;潘孝硕,待发表.
13 Dreirach, O.; Evans, R.; Jguentherodt, H.; Ukuenzi, H., J. Phys. F: Met. Phys., 2(1972) , 709.
14 Evans, R.; Greenwood, D. A.; Lloyd, P., Phys. Lett., 35A(1971) , 57.
15 Cote, P. J.; Meisel, L. V., Phys. Rev. lett,, 39(1977) , 102.
16 Nagel, S. R., Phys. Rev. B, 16(1977) , 1694.
17 Chou, C. P., Phys. Rev. Lett., 37(1976) , 1004.
No related articles found!