OBSERVATIONS ON VOIDS NUCLEATION AND GROWTH IN LOW CARBON STEEL
ZHANG Yizeng (Huazhong Institute of Technology; Wuhan)
Cite this article: 

ZHANG Yizeng (Huazhong Institute of Technology; Wuhan). OBSERVATIONS ON VOIDS NUCLEATION AND GROWTH IN LOW CARBON STEEL. Acta Metall Sin, 1983, 19(1): 70-75.

Download:  PDF(873KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Some observations of voids formation were carried out by using low carbon steel with three kinds of heat-treatment, namely, normalizing, annealing and spheroidizing. Based on these observations and computations, some analytical results have been made to show strain dependency of voids nucleation rate and voids growth rate.
Received:  18 January 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I1/70

1 Puttick, K. E., Philos. Mag., 4(1959) , 964.
2 Beachcm, C. D., ASM Trans. Q., 56(1963) , 318.
3 McClintok, F. A., Trans. ASME, Ser. E: J. Appl. Mech., 35(1968) , 363.
4 Rice. J. R.; Tracey, D. M.; J. Mech. Phys. Solids, 17(1969) , 201.
5 Needleman, A., ibid., 20(1972) , 111.
6 Bridgman, P. W., Trans. ASM, 32(1944) , 553.
7 Clausing, P., ASM Trans. Q., 60(1967) , 504.
8 Hillard, J. E., Measurement of Volume in Volume, Quantitative Microscopy, Eds. Dehoff, R. T.; Rhines, F. N., McGraw-Hill, New York, 1968, p. 45.
9 Underwood, E. E., Microstructure and Properties, An Atomic Approach to the Nature and Properties of Materials, Ed. Lask, L. A., John Wiley, New York, 1967, p. 432.
10 Przystupa, M. A.; Stout, M. G.; Courtney, T. H., Metall. Trans. 11A(1980) , 643.
11 Le Roy, G.; Embury, J. D.; Edward, G.; Ashby, M. F., Acta Metall., 29(1981) , 1509.
12 Fisher, J. R.; Gurland, J., Met. Sci.,(1981) , №5, 185.
13 Fisher, J. R.; Gurland, J., Met. Sci.,(1981) , №5, 193.
14 Ohji, K.; Ogura, K.; Mutoh, Y., Proceedings of the International Conference on Strength and Fracture of Materials, Japan, 1976, p.99.
No related articles found!
No Suggested Reading articles found!