COMPUTER SIMULATION OF SEGREGATION IN BINARY SYSTEM CRYSTALLIZATION
HU Zipu; YAO Lianzeng (University of Science and Technology of China; Hefei)
Cite this article: 

HU Zipu; YAO Lianzeng (University of Science and Technology of China; Hefei). COMPUTER SIMULATION OF SEGREGATION IN BINARY SYSTEM CRYSTALLIZATION. Acta Metall Sin, 1983, 19(1): 109-114.

Download:  PDF(432KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Taking two-phase equilibrium point of the single component system as a basic, an expression for kinetic rate constants of the binary system crystallization was derived in consideration of the changes in the chemical potential of gaseous phase and in the bond combination energy of crystalline phase after a new constituent added. The chemical potential differences caused by both partial pressure and equilibrium temperature shift have been taken into account. Hence, it may be available for any binary system with an arbitrary proportion.The computer simulation was made of the crystallization process for binary systems. It was shown that when the bond between molecules A and B is weaker than that between two A's, the segregation coefficients will be smaller than 1, adding of the new constituent makes the growth slower, and then the chemical potential of vapour must be increased to obtain the equilibrium with crystalline phase. In contrast to this, when the bond between A and B is stronger than that between two A's, the segregation coefficients will be greater than 1, adding of the new constituent makes the growth faster, and then the chemical potential of the vapour must be decreased to obtain the equilibrium with crystalline phase. In both cases, with the increasing growth rate, the segregation coefficients will approach to 1 more and more.All the simulation results seem to be in accordance with the binary system phase diagram and the model seems to be considered correctly.
Received:  18 January 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I1/109

1 Gilmer, G. H., J. Cryst. Growth, 42(1977) , 3.
2 Gilmer, G. H.; Jackson, K. A., 1976 Crystal Growth and Materials, eccg-1 Zurich, Eds. Kaldis, E.; Scheel, H. J., North-Holland, Amsterdam, 1977, p. 79.
3 Muller-Krumbhaar, H., Monte-Carlo Methods in Statistical Physics, Ed. Binder, K., Sprinser-Verlag, Berlin, 1979, p. 290.
4 Gilmer, G. H.; Bennema, P., J. Cryst. Growth, 13/14(1972) , 148.
5 Leamy, H. J.; Gilmer, G. H.; Jackson, K. A., Surface Physics of Materials, Ed. Blakely, J. M., Academic Press, New York, 1975, p. 121.
6 郑兆勃;胡兹莆,物理,10(1981) ,368._
No related articles found!
No Suggested Reading articles found!