PHASE AND STRUCTURE TRANSFORMATION OF BAINITE IN 3Cr3Mo3VNb STEEL DURING TEMPERING
FENG Ganjiang; SHEN Fengqi; CHEN Mingmo (North-Westen Polytechnical University; Xi'an)
Cite this article: 

FENG Ganjiang; SHEN Fengqi; CHEN Mingmo (North-Westen Polytechnical University; Xi'an). PHASE AND STRUCTURE TRANSFORMATION OF BAINITE IN 3Cr3Mo3VNb STEEL DURING TEMPERING. Acta Metall Sin, 1983, 19(2): 23-148.

Download:  PDF(2719KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The phase and structure transformation of bainite during tempering after isothermal quenching were studied on steel 3Cr3Mo3VNb. It was shown that the secondary hardening of bainite is similar to martensite, mainly formed by precipitation of fine dispersed carbides such as Mo_2C, V_4C_3, NbC, etc. The slow dissolution of coarse cemetite in bainite retards the precipitation rate of carbides during tempering. The decomposition and transformation of the retained austenite in bainite differ from that in martensite. The lower dislocation density in bainite is unfavourable for the aggregation and coarsening of carbides. As a result of the coaction of abovementioned factors, the bainite has superior secondary hardening effect, thermal strength and structural stability to martensite formed by straight tempering.
Received:  18 February 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I2/23

1 Jatczk, C. F., ASM Trans. Q., 58(1965) , 195.
2 Simcoe, C. R.; Nehrenbery, A. E., ASM Trans. Q., 58(1965) , 378.
3 Tunney, R. J.; Ridley, N., Met. Sci., 13(1979) , 585.
4 Tunney, R. J.; Lorimer, G. W.; Ridley, N., Met. Sci., 12(1978) , 271.
5 Inoue, A.; Masumoto, T., Metall. Trans., 11A(1980) , 739.
6 Raynor, D.; Whiteman, J. A.; Honeycombe, R. W. K,, J. Iron Steel Inst., 204(1966) , 349.
7 Hopkin, L. M. T.; Jenkinson, E. A., J. Iron Steel Inst., 202(1964) , 929.
8 西田卓彦;谷野满,日本金属学会志,29(1965) ,728.
9 Smith, R.; Iron Steel Inst. Spec. Rep., №64(1959) , 307.
10 Nutting, J., J. Iron Steer Inst., 207(1969) , 872.
11 Hippsley, C. A., Met. Sci., 15(1981) , 137.
12 Seal, A. K.; Honeycombe, R. W. K., J. Iron Steel Inst., 188(1958) , 343.
13 Ridal, K. A.; Quarrell, A. G., J. Iron Steel Inst., 200(1962) , 359.
14 Lupton, J. B.; Murphy, S.; Woodhead, J. H., Metall. Trans., 3A(1972) , 2923.
15 Schulz, B. J.; McMahon, C. J., Jr., Metall. Trans., 4A(1973) , 2485.
No related articles found!