| AN INVESTIGATION ON Sr MODIFICATION OF AN Al-Si-Cu-Mg ALLOY |
| by MAO Xiaoyu; CHEN Jisen; WU Zuanxian; WANG Caoyuan (Nei Monggol Institute of Metallic Materials; Baotou) |
|
Cite this article:
by MAO Xiaoyu; CHEN Jisen; WU Zuanxian; WANG Caoyuan (Nei Monggol Institute of Metallic Materials; Baotou). AN INVESTIGATION ON Sr MODIFICATION OF AN Al-Si-Cu-Mg ALLOY. Acta Metall Sin, 1983, 19(3): 60-156.
|
|
|
Abstract The Sr modification of an Al-Si-Cu-Mg hypoeutectic cast alloy has been investigated by using SEM with both wavelength and energy dispersive X-ray spectrometers. It is found that the Sr addition does not affect the size of Al-Si eutectic cells in the alloy, but changes the morphology of eutectic Si. Hence, the Sr modification is resulted not by the change in nucleation of eutectic Si, but by that in mode of its growth. An available new idea "modification threshold value" was also proposed.
|
|
Received: 18 March 1983
|
1 Hess, P. D.; Blackmun, E. V., Trans. Am. Foundrymen's Soc., 83 (1975) , 87. 2 Davimi, P.; Ghafelehbashi, M., Br. Foundryman, 72 (1979) , 4. 3 Leandro,L.M.,et al.,第43届国际铸工会议论文集,沈阳铸造研究所编译,1979,p.40. 4 Holmanova, M., Prakt. Metallogr., 11 (1974) , 155. 5 Reznick, P.; Stetina, K., ibid., 16 (1979) ,59. 6 Paul, J.; Muerrle, U., ibid., 18 (1981) , 413. 7 徐祖耀,金属学原理,上海科学技术出版社,1964. 8 Mondolfo, L. F1. , Aluminium Alloys: Structure and Properties, Butterworth, London, 1976, p.677. 9 赵志国;杨书祥,大连工学院学报,20(1981) ,55. 10 Day, M. G., J. Inst. Met., 98 (1970) , 57. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|