| ON THE ZERO CHARGE POTENTIALS OF SOLID METAL ELECTRODES IN MOLTEN SALT |
| by PENG Ruiwu; ZHANG Junyue (Shanghai Institute of Metallurgy; Academia Sinica) |
|
Cite this article:
by PENG Ruiwu; ZHANG Junyue (Shanghai Institute of Metallurgy; Academia Sinica). ON THE ZERO CHARGE POTENTIALS OF SOLID METAL ELECTRODES IN MOLTEN SALT. Acta Metall Sin, 1983, 19(3): 72-76.
|
|
|
Abstract The double layer capacitances and zero charge potentials of certain solid metal electrodes in LiCl-KCl melts at 450℃ have been measured by an A. C. bridge method. The zero charge potentials, ε, for Pt, Ag, Cu and Al electrodes are +0.2, -0.4, -0.6 and -1.0 V respectively which was estimated by the minima of C-V curves. If these data together with selected ones from published works in NaCl-KCl melt at 700℃ plotted against their own ionization free energy, △Z_2, a straight line, paralleled that in aqueous solution, may be drawn and expressed as:ε=0.305(△Z_2/q)+Awhere q——1 mole electron charge and A——constant.It indicates that the zero charge potentials between two chlorides molten salt are alike of same solid metals but differ of different ones, and their difference is similar to that in aqueous solution. Thus, it seems to be proposed that the zero charge potentials of the solid metals in molten salts are only determined by the nature of metals themself.
|
|
Received: 18 March 1983
|
1 #12 2 #12 3 Imman, D.; Graves, A. D.; Sethi, R. S., Eletrochemistry, Vol. 1, A Review of the Literature, Alden and Mowbray Ltd, 1970, p. 166. 4 #12 5 彭瑞伍;张俊岳,全国第一次冶金过程物理化学学术报告会论文集,上海科学技术出版社,1965,p.528. 6 Hill, G. J.; Johnson, K. E., J. Electrochem Soc., 108 (1961) , 1013. 7 Blander, M., Molten Salts Chemistry, Interscience Publ., 1964, p. 715. 8 Ukshe, E. A.; Bukuh, N. G.; Leik, S. D. I.; Fumkin, A. N., Electrochem. Acta, 9 (1964) , 431. 9 #12 10 Handbook of Chemistry and Physics, 58th ed., Ed. Robert, C. W., Cleveland, Ohio, 1977, p. E81-81. 11 #12 12 Peng Ruiwu (彭瑞伍); Pang Yongxou (逄永秀); Chen Tzuyao (陈自姚); Zhang Juyue (张俊岳), Preprint of First China-USA Bilateral Metallurgical Conf., Beijing, China, 1981, p. 108. 13 熔盐电化学,彭瑞伍译,上海科学技术出版社,1964. p.200. |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|