SEGREGATION OF S AND P ALONG GRAIN BOUNDARY IN HIGH SPEED STEELS AND CLEANING ACTION OF RE ELEMENTS
by LUO Di; XING Guohua (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing); ZOU Huiliang; YAN Shensheng; YU Zhizhong; LUO Xinghua (Shanghai Institute of Test Technics) (Manuscript received 20 January; 1982; revised manuscript 3 January; 1983)
Cite this article: 

by LUO Di; XING Guohua (Central Iron and Steel Research Institute; Ministry of Metallurgical Industry; Beijing); ZOU Huiliang; YAN Shensheng; YU Zhizhong; LUO Xinghua (Shanghai Institute of Test Technics) (Manuscript received 20 January; 1982; revised manuscript 3 January; 1983). SEGREGATION OF S AND P ALONG GRAIN BOUNDARY IN HIGH SPEED STEELS AND CLEANING ACTION OF RE ELEMENTS. Acta Metall Sin, 1983, 19(4): 121-126.

Download:  PDF(761KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The segregation of the impurities, e. g. S, P, along grain boundaries of as-cast structure and of austenite in the high speed steels as well as the cleaning action of RE elements have been studied by AES. It was found that the more S and P the steels contain, the more their segregation occurs. The segregation becomes remarkably improved by the addition of RE elements, and the enrichment of S at grain boundary goes so far as to vanish when the RE added up to 0.05-0.08%. Some discussion on the segregation and the cleaning action have been also made.
Received:  18 April 1983     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1983/V19/I4/121

1 Oudar, J., Int. Met. Rev., 23 (1978) , 57.
2 Hondros, E. D.; Seah, M. P., Int. Met. Rev., 22 (1977) , 262.
3 罗迪;邢国华;邹惠良;金属学报,19(1983) .
4 Seah, M. P.; Hondros, E. D., Proc. R. Soc. Lond., A335 (1973) , 191.
5 飯田修一;大野和郎;神前熙;熊谷宽夫;泽田正二,物理学常用数表,张质贤等译,科学出版社,1979,p.19.
6 Mulford, R. A.; McMahon, C. J., Jr.; Pope, D. P.; Feng, H. C., Metall. Trans., 7A (1976) , 1183.
7 Olefjord, I., Int. Met. Rev., 23 (1978) , 149.
8 Stein, D. F.; Heldt, L. A., Interfacial Segregation, Eds. Johnson, W. C.; Blakely, J. M., ASM Metals Park, Ohio, 1979, p.239.
No related articles found!
No Suggested Reading articles found!