INTERACTION BETWEEN A1-Si FILLER METAL AND BASE METAL FOR ALUMINUM BRAZING
CHEN Gengbao; WU Jinhua; LI Geyang (Shanghai Jiaotong University) (Manuscript received 30 July; 1983)
Cite this article: 

CHEN Gengbao; WU Jinhua; LI Geyang (Shanghai Jiaotong University) (Manuscript received 30 July; 1983). INTERACTION BETWEEN A1-Si FILLER METAL AND BASE METAL FOR ALUMINUM BRAZING. Acta Metall Sin, 1984, 20(3): 277-279.

Download:  PDF(2084KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The interaction between Al-Si eutectic filler metal and base metal in keeping the fillet at brazing temperature has been studied. It was shown that the interaction is mainly the solution of base metal into filler metal, and the diffusion of filler metal through the grain boundary of base metal has not been observed yet.
Received:  18 March 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I3/277

1 陈根宝;吴锦华;李戈扬,上海交通大学八十七周年校庆论文,1983.
2 张启运;刘淑祺,金属学报,17(1981) ,300.
3 Mondolfo, L. F., Aluminum Alloy: Structure and Properties, London, Butterworths, 1976, p. 661.Z
No related articles found!
No Suggested Reading articles found!