RELATIONSHIP BETWEEN SALTING-OUT EFFECT AND EXTRACTION MECHANISM DURING SOLVENT EXTRACTION OF TRANSITION METALS BY AMINES
YU Shuqiu; CHEN Jiayong (CHEN Chia-yung) (Institute of Chemical Metallurgy; Academia Sinica; Beijing) (Manuscript received 28 June; 1983)
Cite this article: 

YU Shuqiu; CHEN Jiayong (CHEN Chia-yung) (Institute of Chemical Metallurgy; Academia Sinica; Beijing) (Manuscript received 28 June; 1983). RELATIONSHIP BETWEEN SALTING-OUT EFFECT AND EXTRACTION MECHANISM DURING SOLVENT EXTRACTION OF TRANSITION METALS BY AMINES. Acta Metall Sin, 1984, 20(6): 448-457.

Download:  PDF(662KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effect of the presence of inorganic salts in aqueous phase on solvent extraction of metals by an extractant could be different during extraction with different mechanisms. The salting-out effect of the extraction of W(Ⅵ), MoⅥ),V(Ⅴ) and Cr(Ⅵ) by amines under anion-exchange and solvation mechanisms respectively was studied. During solvation extraction of oxyacids of transition metals by amines, hydrophilic complexes were formed first between them. The formation of these complexes depends greatly on the activity of water molecules in the aqueous phase. The addition of inorganic salts to the aqueous phase will decrease the activity of water molecules and thus decrease the extraction of metals into the organic phase. However, during extraction of metals by amine salts with anion-exchange mechanism, the presence of inorganic salts will diminish or prevent the formation of hydrophilic complexes in the simultaneous side reaction and thus increase the percent of metals extracted by the main anion-exchange reaction. Therefore, the extraction of transition metals by amines can be increased or decreased by the addition, of inorganic salts to the aqueous phase with anion-exchange and solvation extraction mechanisms respectively. Some new viewpoints about salting-out effect in solvent extraction were proposed.
Received:  18 June 1984     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1984/V20/I6/448

1 萃取平衡的物理化学,萃取論文集(下),孙彦昕;邓佐卿;毕木天译,中国工业出版社,1965,p.1-82.
2 盐析现象的分子动力学性质,萃取論文集(下),孙彦昕;邓佐卿;毕木天译,中国工业出版社,1965,p.228-230.
3 Eger, I., Proc. Int. Solvent Extration Conf., Vol.2, Ed. Jeffreys, G. V., Soc Chem. Ind., London, 1973, p.1730.
4 Kertes, A. S., The Chemistry of Solvent Extraction in "Recent Advences in Liquid-Liquid Extraction," Ed. Hansen, C., Pergamon, Press, Oxford, Endland, 1971, p. 15-72.
5 Van Ooyen, J., Solvent Extraction Chemsitry, Ed. Dyrssen, D., North-Holland, Amsterdam, 1967, p. 485-492.
6 麦若夫,萃取手册 第二卷,A.M.罗津主编,袁承业等译,原子能出版社,1982,p.159.
7 于淑秋;孟祥胜;陈家镛,中国科学,B辑,(1982) ,11.
8 于淑秋;陈家镛,金属学报,18(1982) ,187.
9 于淑秋;陈家镛,金属学报,20(1984) .
10 马荣骏编著,溶剂萃取在湿法冶金中的应用,冶金工业出版社,1979,p.12-24.
No related articles found!
No Suggested Reading articles found!