Please wait a minute...
Acta Metall Sin  1985, Vol. 21 Issue (1): 25-33    DOI:
Current Issue | Archive | Adv Search |
SNOEK-KSTER RELAXATION IN Ta-O
LI Guangyi;PAN Zhengliang Institute of Metal Research;Academia Sinica;Shenyang;ZHANG Jinxiu Department of Physics;Sun Yat-sen University;Guangzhou
Cite this article: 

LI Guangyi;PAN Zhengliang Institute of Metal Research;Academia Sinica;Shenyang;ZHANG Jinxiu Department of Physics;Sun Yat-sen University;Guangzhou. SNOEK-KSTER RELAXATION IN Ta-O. Acta Metall Sin, 1985, 21(1): 25-33.

Download:  PDF(663KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The Snoek-Kster relaxation processes in oxygen-doped high purity polycrys-talline Ta after plastic deformation were investigated.It was shown that there arefour distinct types of Snoek-Kster relaxation,namely,SK-1 and SK-2 occurringin lower oxygen concentration,i.e.,unsaturated interstitial atmosphere,as sameas peak(1)and(2)in the previous work by the authors;SK-4 in high oxygenconcentration,i.e.,saturated atmosphere and SK-5 in lower oxygen concentration,i.e.,unsaturated atmosphere.The activation parameters of these relaxations weredetermined.As the increasing of the annealing temperature and oxygen content,the gradual transition from SK-5 into SK-4 relaxation can be observed.All relax-ation processes other than SK-1 are stable on annealing.A comparison of resultsbetween previous works and this study was also made.
Received:  18 January 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I1/25

1 潘正良;张进修;李广义,金属学报,21(1985) .
2 Seeger,A.;Weller,M.;Diehl,J.;Pan,Z.L.(潘正良);Zhang,J.X.(张进修),K,T.S.(葛庭燧),Z.Metallk.,73(1982) ,1.
3 Schoeck,G.;Mondino,M.,J.Phys.Soc.Jpn.,18(1963) ,Suppl.1,149.
4 De Lamotte,E.;Wert,C.A.,J.Phys.Soc.Jpn.,19(1964) ,1560.
5 Van Ooijen,D.J.;Van der Goot,A.S.,Philips Res.Rep.,22(1967) ,150.
6 Delobelle,P.;Oytana,C.;Varchon,D.,Mater.Sci.Eng.,29(1977) ,261.
7 Oytana,C.;Varchon,D.,Acta Metall,27(1979) ,17.
8 Rodrian,U.;Schultz,H.,Z.Metallk.,73(1982) ,21.
9 Schulze,K.,J.Met.,33(1981) ,№ 2,33.
10 张进修;潘正良,金属学报,21(1985) ,待发表.
No related articles found!