THE FINITE ELEMENT ANALYSIS OF HEAT FIELD OF METAL SHEET DURING ELASTIC-PLASTIC DEFORMATION
LI Shouxin;HUANG Yi;SHI Changxu(C.H.Shih)Institute of Metal Research;Academia Sinica;Shenyang
Cite this article: 

LI Shouxin;HUANG Yi;SHI Changxu(C.H.Shih)Institute of Metal Research;Academia Sinica;Shenyang. THE FINITE ELEMENT ANALYSIS OF HEAT FIELD OF METAL SHEET DURING ELASTIC-PLASTIC DEFORMATION. Acta Metall Sin, 1985, 21(1): 101-109.

Download:  PDF(893KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The temperature distribution all over the metal thin sheet in the process ofelastic-plastic deformation was evaluated by the finite element analysis.With anassumption of almost lack of variance in thermal conductivity during less deforma-tion,the results of the heat field calculated from the finite element analysis usingKelvin's equation of thermal conductivity is in better agreement with that surveyedby an infrared camera.This calculation seems to be available for the thermal effectcaused by elastic-plastic deformation.
Received:  18 January 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I1/101

1 Williams,J.G.,Appl.Mater.Res.,4(1965) ,№ 2. 104.
2 Weichert,R.;Schoenert,K.,J.Mech.Phys.Solids,22(1974) ,127.
3 Fung,Y.C.,Foundation of Solid Mechanics,London,Prentice-Hill Inc.,1965,p.388.
4 Dunlap,R.W.;Hucke,E.E.;Ragone,D.V.,Exp.Mech.,8(1968) ,№ 4,154.
5 Huang,Y.(黄毅);Li,S.X.(李守新);Shih,C.H.(师昌绪),to be presented in Sixth Int.Conf.on Fracture,1984.
6 Nabarro,F.R.N.,Theory of Crystal Dislocation,Oxford University Press,U.S.A.,1967,p.692.
7 Tay,A.O.;Oxley,P.L.B.,Finite Element Methods in Engineering,Proc.1976 Int.Conf.on Finite Element Methods in Engineering,Australia,1976,p.42. 1-42. 21.
8 Marcal,P.V.;King,I.P.,Int.J.Mech.Sci.,9(1967) ,№ 3,143.
9 李大潜等编,有限元素法续讲,科学出版社,1979,p.191.
10 华东水利学院,弹性力学的有限元法,水利水电出版社,1978,p.88./