THERMODYNAMICS(KRC MODEL)OF THE BAINITIC TRANSFORMATION IN Fe-C ALLOYS
XU Zuyao(T.Y.Hsu);MOU Yiwen Shanghai Jiaotong University
Cite this article: 

XU Zuyao(T.Y.Hsu);MOU Yiwen Shanghai Jiaotong University. THERMODYNAMICS(KRC MODEL)OF THE BAINITIC TRANSFORMATION IN Fe-C ALLOYS. Acta Metall Sin, 1985, 21(2): 13-24.

Download:  PDF(818KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  By application of the improved KRC model for determination of △G~(γ→α),the total driving forces for transformation and driving forces for growth(nucle-ation)for the several possible mechanisms of the bainitic transformation in Fe-Calloys,i.e.,γ→α+γ_1,γ→α+Fe_3C and γ→α′(the same composition)and α′→Fe_3C+α_B(the composition of the bainitic ferrite)are calculated.The driving forceof γ→α+Fe_3C is the largest,followed by that of γ→α+γ_1 and that of γ→α′isthe smallest.The driving force for growth of γ→α′is far less than that of γ→α+γ_1.At the temperature range of bainite formation,the driving force for γ→α′ismuch lower than that required for shear mechanism.The driving force for trans-formation of γ→α+γ_1 in 0.1—0.55 wt-%C alloys at B_s temperature is onlyabout -45 J·mol~(-1).At the upper limit temperature of bainite formation,the driv-ing force of γ→α′in 0.8 wt-%C alloy-is about 137 J·mol~(-1),and that of α′→α_B+Fe_3C is—527 J·mol~(-1).If cementite precipitates from the bainitic ferrite,thetotal driving force,i.e.,the sum of the driving forces of the above two processesis only about -390 J·mol~(-1).The above results show that the formation of thebainitie ferrite by shear mechanism is thermodynamically impossible.
Received:  18 February 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I2/13

1 Kaufman,L.;Radcliffe,S.V.;Cohen,M.,Decomposition of Austenite by Diffusional Processes,Eds.Zackey,V,F.;Aaronson,H.I.,Interscience,New York,1962,p.313.
2 Hehemann,R.F.,Phase Transformations,ASM,Metal Park Ohio,1970,p.397.
3 Hehemann,R.F.;Kinsman,K.R.;Aaronson,H.I.,Metall.Trans.,3(1972) ,1077.
4 Aaronson,H.I.;Hall,M.G.;Barnett,D.M.;Kinsman,K.R.Scr.Metall.,9(1975) ,705.
5 Bhadeshia,H.K.D.H.;Edmonds,D.V.,Acta Metall.,28(1980) ,1265.
6 Lacher,J.R.,Proc.Cambridge Philos.Soc.,33(1937) ,518.
7 Fowler,R.H.;Guggenhiem,E.A.,Statistical Thermodynamics,Cambridge University Press,New York,1939,p.442.
8 McLellan,R.B.;Dunn,W.W.,J.Phys.Chem.Solids,30(1969) ,2631.
9 Shiflet,G.J.;Bradley,J.R.;Aaronson,H.I.,Metall.Trans.,9A(1978) ,999.
10 Aaronson,H.I.;Domain,H.A.;Pound,G.M.,Trans.Metall.Soc.AIME,236(1966) ,753.
11 Bhadeshia,H.K.D.H.,Met.Sci.,14(1980) ,230.
12 Lobo,J.A.;Greiger,G.H.,Metall.Trans.,7A(1976) ,1347.
13 Kaufman,L.;Clougherty,E.V.;Weiss,R.J.,Acta Metall.,11(1963) ,323.
14 Mogutnov,B.M.;Tomilin,I.A.;Shvartsman,L.A.,Thermodynamics of Fe-C Alloys,Metallurgy Press,Moscow,1972,p.109.
15 Orr,R.L.;Chipman,J.,Trans.Metall.Soc.AIME,239(1967) ,630.
16 徐祖耀,马氏体相变与马氏体,科学出版社,北京,1980,p.258.
17 徐祖耀,金属材料热力学,科学出版社,北京,1981,p.279-280.
18 Bhadeshia,H.K.D.H.,Met.Sci.,16(1982) ,159.
19 Steven,W.;Haynes,A.G.,J.Iron Steel Inst,London,183(1956) ,349.
20 Hsu,T.Y.(Xu Zuyao);Chang Hongbing,Acta.Metall.,32(1984) ,343.
21 Ko,T.;Cotrell,S.A.,J.Iron Steel Inst.,London,172(1952) ,307.
No related articles found!
No Suggested Reading articles found!