| BEHAVIOUR OF SECONDARY RECRYSTALLIZATION IN ORIENTED Si STEEL CONTAINING VARIOUS INHIBITORS |
| HE Zhongzhi;SUN Xuefan;SHU AI Renjie Central Iron and Steel Research Institute;Ministry of Metallurgical Industry;Beijing |
|
Cite this article:
HE Zhongzhi;SUN Xuefan;SHU AI Renjie Central Iron and Steel Research Institute;Ministry of Metallurgical Industry;Beijing. BEHAVIOUR OF SECONDARY RECRYSTALLIZATION IN ORIENTED Si STEEL CONTAINING VARIOUS INHIBITORS. Acta Metall Sin, 1985, 21(2): 32-36.
|
|
|
Abstract A comparison was made of the action of various inhibitors to certain highpermeability oriented Si steels on the behaviour of primary and secondary recrys-tallization.It is shown that the inhibitory action of AlN is superior to that ofMnS.The suitable average diameter of the primary grains is 15—20 or 10—12μm for two-stage or single-stage cold-rolling process respectively.The stability ofprimary recrystallized matrix is more important than primary grain size.The(110)[001]secondary grains nucleated preferentially at about 1/5-1/4 thick beneathsurface layer of the hot-rolled band.Such prior secondary recrystallizationnucleus of the steel containing AlN inhibitor is in pancake-like shape and the graingrowth is anisotropy.However,the secondary grain growth of the steel containingMnS inhibitor is isotropic.It seems that the secondary grains in the neighbourhoodof the identical(110)[001]orientation may grow into contact with each otherand coalesce to coarse secondary crystals.
|
|
Received: 18 February 1985
|
1 Littmann,M.F.;Dahlstrom,N.A.,J.Appl.Phys.,49(1978) ,2034. 2 Sakai,T.;Matsuo,M.;Tanino,M.;Shindo,T.;Shiozaki,M.,Proc.of the 6th Int.Conf.on Texture of Materials,Ed.Nagashima Shinichi,The Iron Steel Inst.Jpn,Tokyo,1981,p.938. 3 #12 4 Hu H.(胡郇),Recovery and Recrystallization of Metals,Ed.Himmel,L.,Interscience,New York,1963,p.311. 5 #12 6 Pease,N.C.;Jones,D.W.;Wise,M.H.L.;Hutchinson,W.B.,Met.Sci.,15(1981) ,203. |