Abstract  The effect of P contents on the impact toughness of conventionally heat-treated 30CrMnSiA steel has been investigated by means of a series of impact tests.It was resulted that the impact toughness decreases remarkably with the increas-ing of P contents no less than 0.012wt-%.The observation under SEM and byAuger spectroscopy showed that the grain boundary cracking area and the P seg-regation on grain boundaries increase with the increase of P contents.The P seg-regation toward the grain boundary and the noticeable lowering of low tempera-ture impact toughness may be promoted by slow cooling after tempering.The crit-ical temperature of high temperature temper brittleness of the steel tested seemsto be 550℃.
Received:  18 February 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I2/45

1 McMahon,C.J.,Jr.,Mater.Sci.Eng.,25(1976) ,233.
2 McMahon,C.J.,Jr.;Cianelli,A.K.;Feng,C.,Metall.Trans.,8A(1977) ,1055.
3 Kameda,J.;McMahon,C.J.,Jr.,Metall.Trans.,11A(1980) ,91.
4 Jokl,M.L.;Kameda,J.;McMahon,C.J.,Jr.;Vitek,V.,Met.Sci.,14(1980) ,375.
5 曲哲;郭可信,金属学报,16(1980) ,371.
6 杨亦石;邹惠良,金属学报,19(1983) ,A118.
7 雷廷权;唐之秀;苏梅,金属学报,18(1982) ,485.
8 Griffith,A.A.,Philos.Trans.R.Soc.London,A221(1920) ,163.
9 Orowan,E.,Rep.Prog.Phys.,12(1948) ,185.
10 Hondros,E.D.,Proc.R.Soc.London,286A(1965) ,479.
11 Joshi.A.;Stein,D.F.,Temper Embrittlement of Alloy Steels,ASTM STP 499,1973,p.59.g
No related articles found!
No Suggested Reading articles found!