Acta Metall Sin  1985, Vol. 21 Issue (3): 36-44    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF HYDROGEN ON CYCLIC DEFORMATION BEHAVIOUR OF PURE Ni
HOU Yaoyong;WANG Chongmin;WANG Chunbo Lanzhou University
Cite this article: 

HOU Yaoyong;WANG Chongmin;WANG Chunbo Lanzhou University. INFLUENCE OF HYDROGEN ON CYCLIC DEFORMATION BEHAVIOUR OF PURE Ni. Acta Metall Sin, 1985, 21(3): 36-44.

Download:  PDF(1865KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Symmetrical push-pull low-cyclic fatigues with constant strain amplitude,ranged from 2.7×10~(-3)to 4.9×10~(-3),were performed on well-annealed commercialpure(99.98%)Ni polycrystalline specimens with grain size about 30-40 μm underhydrogen-charged,hydrogen-free and hydrogen charged-dehydrized respectively.The cyclic peak stresses σ_P,friction stresses σ_F and back stresses σ_B were deter-mined by the fatigue hysteresis loops.It was shown that the σ_P at saturation,theσ_F and the hardening rate as well as the total fatigue life decreased remarkably withincreasing of strain amplitude but σ_B changed no more under hydrogen-charged.The influence of hydrogen on the cyclic deformation behaviour of pure Ni hasalso been discussed in combination with the SEM observation.
Received:  18 March 1985     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1985/V21/I3/36

1 Kuhlmann-Wilsdorf,D.;Laird,C.,Mater.Sci.Eng.,37(1979) ,111.
2 Lee,J.-K.;Laird,C.,Mater.Sci.Eng.,54(1982) ,53.
3 Boniszewski,T.;Smith,G.C.,Acta Metall.,11(1963) ,165.
4 Eastman,J.;Matsumoto,T.;Narita,N.;Heubaum,F.;Birnbaum,H.K.,Hydrogen Effects in Metals,Proc.of the 3rd Int.Conf.,Wyoming,1981,Eds.Bernstein,I.M.;Thompson,A.W.,AIME,New York,1981,p.397.
5 Matsui,H.;Kimura,H.;Moriya,S.,Mater.Sci.Eng.,40(1979) ,207.
6 Essmann,U.;G(o|¨)esele,U.;Mughrabi,H.,Philos.Mag.,A44(1981) ,405.
7 Polak,J.,Czech.J.Phys.,B23(1973) ,322.
8 Johnson,H.H.;Lin,R.W.,Hydrogcn Effects in Metals,Proc.of the 3rd Int.Conf.,Wyoming,1981,Eds.Bernstein,I.M.;Thompson A.W.,AIME,New York,1981,p.3.
9 Tien,J.K.;Nair,S.V.;Jensen,R.R.,ibid.,p.37.Q
No related articles found!
No Suggested Reading articles found!